RTP 299 X 63548

Category: Nylon 66 , Polyamide 66
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: xfWSGo_RTP-299-X-63548.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Unreinforced - Flame Retardant - Halogen Free - UL94 V-0
General Information
Features
  • Halogen-free
  • Flame retardancy
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.18g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)1.4 - 1.8%ASTM D955
Water Absorption (23°C, 24 hr)0.95%ASTM D570
Moisture Content 0.20%
HardnessNominal ValueUnitTest Method
Rockwell Hardness (R-Scale)118ASTM D785
MechanicalNominal ValueUnitTest Method
Tensile Modulus 4140MPaASTM D638
Tensile Strength 75.8MPaASTM D638
Tensile Elongation (Yield)> 10%ASTM D638
Flexural Modulus 3790MPaASTM D790
Flexural Strength 124MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)43J/mASTM D256
Unnotched Izod Impact (3.20 mm)960J/mASTM D4812
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load ASTM D648
    0.45 MPa, not annealed 188°CASTM D648
    1.8 MPa, not annealed 71.1°CASTM D648
ElectricalNominal ValueUnitTest Method
Volume Resistivity > 1.0E+15ohms·cmASTM D257
FlammabilityNominal ValueUnitTest Method
Flame Rating (0.800 mm)V-0UL 94
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 4.0hr
Dew Point -17.8°C
Processing (Melt) Temp 243 - 277°C
Mold Temperature 65.6 - 107°C
Injection Pressure 68.9 - 124MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
RTP EMI 2563 RTP Company PC+ABS RTP
Tecnoprene® 3K6 NERO903 SO.F.TER. SPA PP Copolymer Tecnoprene®
Zelux® SD-P Westlake Plastics Company PC Zelux®
Hostacom X G3 U12 LyondellBasell Industries PP Copolymer Hostacom
TechnoMid PA6 S SZ TechnoCompound GmbH Nylon 6 TechnoMid