DOW™ LDPE 5004I

Category: LDPE , Low Density Polyethylene Resin
Manufacturer: The Dow Chemical Company
Trademark: DOW™ LDPE
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: kvMdtW_DOW-LDPE-5004I.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Dow LDPE 5004I is used for fresh milk cartons, liquid/juice containers, dry foods packaging, snack foods packaging, moist foods packaging, and medical packaging. Dow LDPE extrusion coating resins provide optimal neck-in and draw-down performance with minimal taste/odor contribution.

  • A low melt index coating resin for demanding packaging applications

Complies with:
  • U.S. FDA 21 CFR 177.1520 (c) 2.2
  • U.S. FDA -DMF
  • Canadian HPFB No Objection (With Limitations)
  • EU, No 10/2011
  • Japan Hygienic Olefin and Styrene Plastics Association
Consult the regulations for complete details.

General Information
Agency Ratings
  • DMF not rated
  • FDA 21 CFR 177.1520(c) 2.2
  • HPFB (Canada) No Objection 2
  • JHOSPA not rated
  • Europe No 10/2011
Forms
  • Particle
Processing Method
  • Extrusion coating
  • cast film
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.924g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)4.2g/10 minASTM D1238
MechanicalNominal ValueUnitTest Method
Coefficient of Friction 1(with self-dynamic, extrusion coating)0.45ASTM D1894
FilmsNominal ValueUnitTest Method
Film Thickness - Tested 25µm
Film Puncture Resistance (25 µm)2.32J/cm³Internal method
Film strength ASTM D882
    MD : 25 µm, cast film 114J/cm³ASTM D882
    TD : 25 µm, cast film 145J/cm³ASTM D882
Tensile Strength ASTM D882
    MD : Yield, 25 µm, extruded film 14.8MPaASTM D882
    TD : Yield, 25 µm, extruded film 10.9MPaASTM D882
    MD : Broken, 25 µm, extruded film 31.0MPaASTM D882
    TD : Broken, 25 µm, extruded film 17.0MPaASTM D882
Tensile Elongation ASTM D882
    MD : Broken, 25 µm, extruded film 220%ASTM D882
    TD : Broken, 25 µm, extruded film 610%ASTM D882
Dart Drop Impact (25 µm, Cast Film)27gASTM D1709A
Elmendorf Tear Strength ASTM D1922
    MD : 25 µm, cast film 310gASTM D1922
    TD : 25 µm, cast film 80gASTM D1922
Seal Initiation Temperature 2(25 µm, Extrusion Coating)105°C
Water Vapor Transmission Rate 3(25 µm, Extrusion Coating)0.59g·mm/m²/atm/24 hrASTM F1249
ThermalNominal ValueUnitTest Method
Vicat Softening Temperature 95.0°CASTM D1525
Melting Temperature (DSC) 112°CInternal method
OpticalNominal ValueUnitTest Method
Gloss (45, 25.4 µm, cast film)51ASTM D2457
Haze (25.4 µm, Cast Film)13%ASTM D1003
ExtrusionNominal ValueUnitTest Method
Melt Temperature 316 - 327°C
Neck-in (321°C, 25.4 µm)63.5mmInternal method
Maximum production line speed 7.6m/secInternal method
Minimum coating thickness 7.6µmInternal method
Minimum coating weight 7.2g/m²Internal method
Extrusion instructions
铸造薄膜的制造条件: 螺杆 A,尺寸:2 英寸 (51 mm);30:1 L/D 熔体温度:502°F (261°C) 螺杆速度:33 rpm 螺杆 B,尺寸:2.5 英寸 (63.5 mm); 30:1 L/D 熔体温度:501°F (261°C) 螺杆速度:33 rpm 螺杆 C,尺寸:2.5 英寸 (63.5 mm);30:1 L/D 熔体温度:499°F (259°C) 螺杆速度:33 rpm 螺杆 D,尺寸:2.5 英寸 (63.5 mm);30:1 L/D 熔体温度:500°F (260°C) 螺杆速度:33 rpm 螺杆 E,尺寸:2 英寸 (51 mm);30:1 L/D 熔体温度:501°F (261°C) 螺杆速度:33 rpm 螺杆类型:DSB II 冷却辊温度:70°F (21°C) 生产线速度:400 fpm(123 米/分) 挤出涂层薄膜的制造条件: 螺杆尺寸:3.5 英寸 (89 mm) 30:1 L/D 螺杆类型:带 Maddock Mixer 的单跨型 模具间隙:20 密尔 (0.508 mm) 熔体温度:625°F (329°C) 输出:250 磅/小时 螺杆速度:90 rpm 厚度:1.0 密尔 (25 µm)
Note Message
1 .1.0 Mill (25 µm) coating applied to 50 pounds of kraft paper.
2 .Apply the coating to 50 pounds of kraft paper.
3 .Apply the coating to 50 pounds of kraft paper.
Resin Grade Manufacturer Category Trademark
Shandong PP PMF4201 Shandong Dongchen Engineering Plastics Co., Ltd. PP, Unspecified Shandong PP
Tectron H2295 TECTRON Systems Pte Ltd TPV Tectron