25% glass fibre reinforced flame retardant polyamide 66 (V-0), halogenated, free of PBDE and antimony oxide |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
UL File Number |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.59 | -- | g/cm³ | ISO 1183/A |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 10000 | 8000 | MPa | ISO 527-2/1A/1 |
Tensile Stress (Break) | 150 | 112 | MPa | ISO 527-2/1A/5 |
Tensile Strain (Break) | 2.1 | 3.0 | % | ISO 527-2/1A/5 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 7.0 | -- | kJ/m² | |
23°C | 9.0 | 12 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | 44 | -- | kJ/m² | |
23°C | 52 | 55 | kJ/m² |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, Unannealed | > 250 | -- | °C | ISO 75-2/Bf |
1.8 MPa, Unannealed | 232 | -- | °C | ISO 75-2/Af |
Vicat Softening Temperature | ||||
-- | > 250 | -- | °C | ISO 306/A50 |
-- | 229 | -- | °C | ISO 306/B50 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Comparative Tracking Index (Solution A) | 375 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Rate (2.00 mm) | 0.0 | -- | mm/min | ISO 3795 |
Flammability Classification | IEC 60695-11-10, -20 | |||
0.800 mm | V-0 | -- | ||
1.60 mm | V-0 | -- | ||
3.20 mm | V-0 | -- | ||
Glow Wire Flammability Index | IEC 60695-2-12 | |||
0.500 mm | 960 | -- | °C | |
0.750 mm | 960 | -- | °C | |
1.50 mm | 960 | -- | °C | |
3.00 mm | 960 | -- | °C | |
Glow Wire Ignition Temperature | IEC 60695-2-13 | |||
0.500 mm | 900 | -- | °C | |
0.750 mm | 900 | -- | °C | |
1.50 mm | 900 | -- | °C | |
3.00 mm | 900 | -- | °C | |
Oxygen Index | 34 | -- | % | ISO 4589-2 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RheTech Polypropylene HP513-00 | RheTech, Inc. | PP Copolymer | RheTech Polypropylene |
Borclear™ RC737MO | Borealis AG | PP Random Copolymer | Borclear™ |
Electrafil® ABS A4 | Techmer Engineered Solutions | ABS | Electrafil® |
KOCETAL® WR301GR | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |
Plaslube® PC / ABS 830 | Techmer Engineered Solutions | PC+ABS | Plaslube® |