| Category: | PVC, Unspecified , Polyvinyl Chloride |
| Manufacturer: | Teknor Apex Asia Pacific PTE. LTD. |
| Trademark: | APEX® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | WVAr15_APEX-S94-A0907C2-80NT.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| APEX S94-A0907C2-80NT is a Polyvinyl Chloride NSF Extrusion Compound available in opaque granular form. It complies with NSF/ANSI STANDARD 61. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.37 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 86 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength 1(Break) | 20.0 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 300 | % | ASTM D638 |
| Additional Information |
|---|
| Typical temperature profile for processing compound is from 145°C to 185°C. The optimum temperatures depend on the type of machine as well as screw design being used to process.Feeding zone: 145°CCompression zone: 155°C to 165°CMixing zone: 160°C to 170°CNozzle/ Die zone: 170°C to 185°C |
| Note Message | |
|---|---|
| 1 . | 500 mm/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| tefabloc® TO 223 | Mitsubishi Chemical Performance Polymers, Inc. | TPE | tefabloc® |
| CALSIN 110FRF | Pooya Polymer Tehran | Polyolefin, Unspecified | CALSIN |
| Dryflex® 602600S | ELASTO | SEBS | Dryflex® |
| Fortron® 0320 | Celanese Corporation | PPS | Fortron® |
| RTP 199 X 141363 B | RTP Company | TPO (POE) | RTP |