Elastollan® 695A-15N

Category: TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester)
Manufacturer: BASF Corp. Thermoplastic Polyurethanes
Trademark: Elastollan®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: Vtb3OW_Elastollan-695A-15N.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Elastollan® 695AN is specifically formulated for extruded profile, sheet and film applications. It exhibits excellent abrasion resistance, toughness, high transparency, low gel, and low yellowness index. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® 695AN conforms to the FDA food contact regulations as described in book 21, section 177.2600 and 177.1680 for both wet and dry food contact applications respectively. Elastollan® 695AN is supplied uncolored in pellet form.
General Information
Features
  • Food Contact Acceptable
  • Good Abrasion Resistance
  • Good Tear Strength
  • Good Toughness
  • Low Gel
Agency Ratings
  • FDA 21 CFR 177.1680
  • FDA 21 CFR 177.2600
Appearance
  • Clear/Transparent
Processing Method
  • Extrusion
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.23g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/21.6 kg)20 to 60g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A)94ASTM D2240
MechanicalNominal ValueUnitTest Method
Tensile Modulus (Injection Molded)40.0MPaASTM D412
Flexural Modulus (Injection Molded)44.1MPaASTM D790
Taber Abrasion Resistance 25.0mgASTM D1044
Abrasion - DIN 30mm³DIN 53516
ThermalNominal ValueUnitTest Method
Softening Point - DMA 87°CInternal Method
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% Strain 14.5MPa
    300% Strain 31.7MPa
Tensile Strength 40.7MPaASTM D412
Tensile Elongation (Break)450%ASTM D412
Tear Strength 1149kN/mASTM D624
Compression Set ASTM D395B
    23°C, 22 hr 25%
    70°C, 22 hr 40%
ThermalNominal ValueUnitTest Method
Glass Transition Temperature -18.0°CInternal Method
Vicat Softening Temperature 117°CASTM D1525
InjectionNominal ValueUnit
Drying Temperature 110 to 120°C
Drying Time 2.0 to 3.0hr
Suggested Max Moisture 0.030%
Rear Temperature 190 to 220°C
Middle Temperature 190 to 220°C
Front Temperature 190 to 220°C
Nozzle Temperature 210 to 225°C
ExtrusionNominal ValueUnit
Drying Temperature 110 to 120°C
Drying Time 2.0 to 3.0hr
Cylinder Zone 1 Temp. 170 to 210°C
Cylinder Zone 3 Temp. 170 to 210°C
Cylinder Zone 5 Temp. 170 to 210°C
Adapter Temperature 200 to 220°C
Die Temperature 195 to 215°C
Note Message
1 .Die C
Resin Grade Manufacturer Category Trademark
RTP 105CC HI UV RTP Company PP Copolymer RTP
Sylvin 8225-60 Natural Sylvin Technologies Incorporated PVC, Flexible Sylvin
Chemical Resources PP 1200NW1 Chemical Resources, Inc. PP Homopolymer Chemical Resources
CYCOM® 823 RTM Cytec Industries Inc. Epoxy CYCOM®
SABIC® PPcompound 8611P Saudi Basic Industries Corporation (SABIC) PP, Unspecified SABIC® PPcompound