Staramide BG3C1 is a 15 % Glass Fiber Reinforced Polyamide 6 Injection Molding Resin
General Information
Filler / Reinforcement
  • Glass Fiber, 15% Filler by Weight
RoHS Compliance
  • RoHS Compliant
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Density 1.20g/cm³ISO 1183
Molding Shrinkage - Flow 10.70 to 1.2%Internal Method
MechanicalNominal ValueUnitTest Method
Tensile Modulus 5500MPaISO 527-2/1
Tensile Stress (Break)90.0MPaISO 527-2/5
Tensile Strain (Break)5.0%ISO 527-2/5
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength 2(23°C)12kJ/m²ISO 180/1A
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature 3
    0.45 MPa, Unannealed, 100 mm Span 190°CISO 75-2/Be
    1.8 MPa, Unannealed, 100 mm Span 170°CISO 75-2/Ae
Vicat Softening Temperature 200°CISO 306/A50
ElectricalNominal ValueUnitTest Method
Comparative Tracking Index IEC 60112
    -- 600V
    Solution B 500V
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.60 mm, Tested by E2P)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 75.0 to 85.0°C
Drying Time 4.0 to 6.0hr
Suggested Max Moisture 0.20%
Rear Temperature 230 to 240°C
Middle Temperature 240 to 250°C
Front Temperature 240 to 270°C
Processing (Melt) Temp 240 to 270°C
Mold Temperature 60.0 to 80.0°C
Note Message
1 .Tensile Bar
2 .80*10*4
3 .120*10*4
Resin Grade Manufacturer Category Trademark
RTP 605 FR RTP Company ABS RTP
Medalist® MD-110 Teknor Apex Company TPE Medalist®
TECHNYL® C 30H1 V30 NATURAL/F Solvay Engineering Plastics Nylon 6 TECHNYL® C
Geon™ 210 Series 215 Blending Resin Mexichem Specialty Resins, Inc. PVC Homopolymer Geon™ 210 Series
NYLOY® MS-0100N-SP Nytex Composites Co., Ltd. Nylon 66 NYLOY®