It is a hard, black, UV-resistant thermoplastic vulcanized elastomer (TPV) in the thermoplastic elastomer (TPE) series. This material has good physical properties and chemical resistance at the same time, and is used in fields that are difficult to injection molding. This brand of Shanduping TPV is a shear rate dependent product that can be processed on conventional thermoplastic injection molding equipment. This is a polyolefin-based material that can be recycled in the production process.
General Information
Features
  • Good dimensional stability
  • Good UV resistance
  • Recyclable materials
  • Good formability
  • High liquidity
  • Ozone resistance
  • Good chemical resistance
  • Fatigue resistance
  • Excellent appearance
Uses
  • Parts under the hood of a car
  • Application in Automobile Field
  • Car interior equipment
  • Car exterior decoration
  • Outdoor application
Agency Ratings
  • UL QMFZ2
  • UL QMFZ8
RoHS Compliance
  • RoHS compliance
UL File Number
  • E80017
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Multiple injection molding
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity
    -- 0.908g/cm³ASTM D792
    -- 0.910g/cm³ISO 1183
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shaw A, 15 seconds, 23°C, 2.00mm)91ISO 868
ElastomersNominal ValueUnitTest Method
Tensile Stress - Across Flow (100% Strain, 23°C)4.80MPaASTM D412, ISO 37
Tensile Strength - Across Flow (Break, 23°C)7.30MPaASTM D412, ISO 37
Tensile Elongation - Across Flow (Break, 23°C)390%ASTM D412, ISO 37
Tear Strength - Across Flow
    23°C 131.0kN/mASTM D624
    23°C 231kN/mISO 34-1
Compression Set
    70°C, 22 hr 353%ASTM D395B
    125°C, 70 hr 462%ASTM D395B
    70°C, 22 hr 553%ISO 815
    125°C, 70 hr 662%ISO 815
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air (150°C, 168 hr)3.0%ASTM D573, ISO 188
Change in Ultimate Elongation in Air (150°C, 168 hr)-24%ASTM D573, ISO 188
Change in Durometer Hardness in Air (Shore A, 150°C, 168 hr)1.0ASTM D573, ISO 188
ThermalNominal ValueUnitTest Method
Brittleness Temperature -54.0°CASTM D746, ISO 812
FlammabilityNominal ValueTest Method
Flame Rating (1.10 mm)HBUL 94
Additional Information
如果适用,这是基于扇形浇口注塑成型的平板测试结果。拉伸强度、伸长率和拉伸应力沿垂直流动方向测定 - ISO 1 型,ASTM die C。25% 形变时的永久压缩变形。撕裂强度 - DIN 53515,die C(带缺口)。从埃克森美孚欧洲分支机构直接购买的所有产品都符合 REACH 法规。 对于埃克森 美孚未进口至欧洲的产品,用户应自行评估其是否满足 REACH 法规。
Legal statement
未经埃克森美孚化工书面允许,这种产品包括其产品名称,不得在任何医疗应用领域予以使用或有关详细的产品监管信息,请联系客户服务。
Injection instructions
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《注射成型指南》。
Note Message
1 .C mould
2 .Method B, right-angle specimen (cut)
3 .Type 1
4 .Type 1
5 .Type a
6 .Type a
Resin Grade Manufacturer Category Trademark
Maxxam™ 34-1520 UV SSM TFPP PolyOne Corporation PP Homopolymer Maxxam™
Tarnoform® 400 Grupa Azoty S.A. Acetal (POM) Copolymer Tarnoform®
Karina IVORY PVC COMPOUND 105911-35/ 1-BY-AC-LMP Karina Ind. e Com. de Plásticos Ltda PVC, Unspecified Karina
Vydyne® R530H BK0713 Ascend Performance Materials Operations LLC Nylon 66 Vydyne®
Sylvin 4280-65UV Black Sylvin Technologies Incorporated PVC, Unspecified Sylvin