| Category: | Acetal (POM) Copolymer , Acetal (POM) Copolymer |
| Manufacturer: | BARLOG plastics GmbH |
| Trademark: | KEBAFORM® C |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | QqT7mW_KEBAFORM-C-6027.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| POM Copolymer, 30% mineral reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Resin ID (ISO 1043) |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.55 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 20 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 5100 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 60.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 8.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 4.0 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength (23°C) | 55 | kJ/m² | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 140 | °C | ISO 75-2/A |
| Melting Temperature 1 | 166 | °C | ISO 11357-3 |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SABIC® Polyester SF 312 | Saudi Basic Industries Corporation (SABIC) | PET | SABIC® HDPE |
| SILVER® PA623G40 | Guangdong Silver Age Sci & Tech. Co., Ltd | Nylon 66 | SILVER® |
| LUVOCOM® 80/TF/18/SI/2 - 1P | Lehmann & Voss & Co. | Acetal (POM) Copolymer | LUVOCOM® |
| Petrothene® FR200000 | LyondellBasell Industries | Polyolefin, Unspecified | Petrothene® |
| SQUARE® LSR2034-45BS | Shenzhen SQUARE Silicone Co., Ltd. | Silicone Rubber, LSR | SQUARE® |