Glass fibre-reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.21 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 1.2 | -- | % | |
Flow | 0.50 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Stress | 120 | 75.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 3.5 | 8.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 4800 | 3300 | MPa | ISO 178 |
Flexural Stress | 180 | 130 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 5.0 | 7.0 | kJ/m² | ISO 179 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature 1 | ||||
0.45 MPa, Unannealed | 230 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 220 | -- | °C | ISO 75-2/A |
Vicat Softening Temperature | > 210 | -- | °C | ISO 306/B50 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (1.60 mm) | HB | -- | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 650 | -- | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Mediprene® 500800M | ELASTO | SEBS | Mediprene® |
Braskem PE HS5407 | Braskem | HDPE | Braskem PE |
HiFill® PP 0159 | Techmer Engineered Solutions | PP, Unspecified | HiFill® |
KYDEX® 6565(d) | SEKISUI Polymer Innovations, LLC | PMMA+PVC | KYDEX® |
Pearlthane® 12F75UV | Lubrizol Advanced Materials, Inc. | TPU-Polyester | Pearlthane® |