Chemlon® 214 GH is a Polyamide 6 (Nylon 6) material filled with 14% glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Important attributes of Chemlon® 214 GH are:
Typical application of Chemlon® 214 GH: Automotive |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.23 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 0.50 to 1.0 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 114 | MPa | ASTM D638 |
Tensile Elongation | ASTM D638 | ||
Yield | 3.0 | % | |
Break | 3.0 | % | |
Flexural Modulus | 4310 | MPa | ASTM D790 |
Flexural Strength | 162 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 64 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, Unannealed | 204 | °C | |
1.8 MPa, Unannealed | 188 | °C | |
Melting Temperature | 216 | °C | |
CLTE - Flow | 5.5E-5 | cm/cm/°C | ASTM D696 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+14 | ohms·cm | ASTM D257 |
Dielectric Strength (3.00 mm) | 11 | kV/mm | ASTM D149 |
Comparative Tracking Index (CTI) | 500 | V | UL 746 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (0.810 mm) | HB | UL 94 | |
Oxygen Index | 22 | % | ASTM D2863 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Suggested Max Moisture | 0.20 | % | |
Suggested Max Regrind | 25 | % | |
Rear Temperature | 218 to 235 | °C | |
Middle Temperature | 241 to 257 | °C | |
Front Temperature | 246 to 268 | °C | |
Nozzle Temperature | 246 to 268 | °C | |
Processing (Melt) Temp | 249 to 266 | °C | |
Mold Temperature | 60.0 to 93.3 | °C | |
Injection Pressure | 34.5 to 138 | MPa | |
Screw Speed | 60 to 120 | rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Moplen EP648N | LyondellBasell Industries | PP Impact Copolymer | Moplen |
THERMOLAST® K TP5VCN (Series: AD1/CS) | KRAIBURG TPE | TPE | THERMOLAST® K |
BP RPP 1209 GR BLK | Buckeye Polymers, Inc. | PP, Unspecified | BP |
HI-ZEX™ 530E | Prime Polymer Co., Ltd. | HDPE | HI-ZEX™ |
POLYfill PPC K20040 | Polykemi AB | PP Copolymer | POLYfill |