| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Politem Plastik Ltd. |
| Trademark: | PAmpellonne® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 639sQC_PAmpellonne-607s.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| All Politem Plastik Polyamide Resins are recycled from Post Industrial Fiber Waste Streams |
| General Information | |
|---|---|
| Recycled Content |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.13 to 1.15 | g/cm³ | ISO 1183 |
| Ash Content | 0.30 to 0.50 | % | ISO 3451-4 |
| Moisture | 0.10 to 0.50 | % | ISO 15512/B |
| Relative Viscosity 1 | 2.50 to 2.70 |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| DSC Analysis | > 97 | % | |
| Titanium Dioxide | < 0.30 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 85 to 100 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | > 2500 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | > 50.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 3.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | 6.0 to 7.0 | kJ/m² | ISO 179/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature (DSC) | 263 to 265 | °C | ISO 3146 |
| Note Message | |
|---|---|
| 1 . | Formic |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxelast® P3945C | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| Sinpolene GPP1620 | Teknor Apex Asia Pacific PTE. LTD. | PP Homopolymer | Sinpolene |
| Taitarex® 861D | Taita Chemical Company, Ltd. | PS (GPPS) | Taitarex® |
| Lupoy® 1303AH-10 | LG Chem Ltd. | PC | Lupoy® |
| LUVOCOM® 1301-8290 | Lehmann & Voss & Co. | PPS | LUVOCOM® |