Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
Manufacturer: | ELASTO |
Trademark: | Dryflex® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 1VK1LS_Dryflex-PS-50R201B.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Dryflex PS 50R201B: Thermoplastic Elastomer Base Material: TPS-SEBS Hardness: 50 IRHD Service Temperature Range: -50°C to 120°C Colour: Black, but can easily be coloured in any shade Presentation: Free flowing pellets that can be processed without predrying when stored under normal conditions Chemical Resistance: Good (excluding organic solvents, aromatic and vegetable oils) Recycling: 100% recyclable Mould Shrinkage (linear): Approx. 0.75 - 2% depending on e.g. shape of the detail and placement of gate Special Features: Meets the requirements of BS EN 681-2-2000, the European Standard EN 681-2, Type WT, elastomeric seals for pipe joints |
General Information | |
---|---|
Features |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.05 | g/cm³ | ISO 2781 |
Molding Shrinkage 1 | 0.75 to 2.0 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A) | 46 | ISO 868 | |
IRHD Hardness | 50 | ISO 48 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ISO 37 | ||
Across Flow : Yield | 8.00 | MPa | |
Flow : Yield | 4.00 | MPa | |
Tensile Elongation | ISO 37 | ||
Across Flow : Break | 900 | % | |
Flow : Break | 760 | % | |
Compression Set 2 | ISO 815 | ||
-10°C, 72 hr | 58 | % | |
23°C, 72 hr | 15 | % | |
70°C, 24 hr | 36 | % | |
Stress Relaxation | ISO 3384 | ||
100 day (2400 hr) : 23°C | 21 | % | |
7 day (168 hr) : 23°C | 15 | % |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Volume - Ozone Resistance | No cracking | ISO 1431-1 |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Service Temperature | -50 to 120 | °C |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Stress (70°C, 168 hr) | 4.5 | % | ISO 37 |
Change in Tensile Strain at Break (70°C, 168 hr) | 4.0 | % | ISO 37 |
Change in Shore Hardness (IRHD, 70°C, 168 hr) | 2.0 | ISO 48 | |
Change in Volume (70°C, 168 hr, in Water) | 1.0 | % | ISO 1817 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 190 to 210 | °C | |
Middle Temperature | 190 to 210 | °C | |
Front Temperature | 190 to 210 | °C | |
Mold Temperature | 15.0 to 50.0 | °C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 150 to 210 | °C | |
Cylinder Zone 2 Temp. | 150 to 210 | °C | |
Cylinder Zone 3 Temp. | 150 to 210 | °C | |
Cylinder Zone 4 Temp. | 150 to 210 | °C | |
Cylinder Zone 5 Temp. | 150 to 210 | °C |
Note Message | |
---|---|
1 . | Depending on shape of the detail and placement of gate |
2 . | Type B |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PPR PPCO08 | Premier Plastic Resins, Inc. | PP Copolymer | PPR |
TROSIFOL® HR100 | Kuraray Co., Ltd. | PVB | TROSIFOL® |
NORDEL™ IP 4820 | The Dow Chemical Company | EPDM | NORDEL™ |
FRAGOM GR/22 PP | Crosspolimeri S.p.A. | Polyolefin, Unspecified | FRAGOM |
HOPELEN SFO-130BA-1 | Lotte Chemical Corporation | PP Homopolymer | HOPELEN |