| Category: | XLPE , Crosslinked Polyethylene |
| Manufacturer: | Borealis AG |
| Trademark: | Borealis |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | zglzDX_Borealis-FR4830.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
FR4830 is a chemically crosslinkable non-halogen flame retardant polyethylene compound for primary automotive and appliance wire. FR4830 is intended for use as a 125°C rated primary insulation for crosslinked automotive and appliance wires. FR4830 meets teh applicable requirements as below when processed using sound extrusion practice and testing procedure:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity 1 | 1.40 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 50 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 16.0 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 220 | % | ASTM D412 |
| Aging | Nominal Value | Unit | |
|---|---|---|---|
| Change in Tensile Strength (168°C, 165 hr) | < -20 | % |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | < -50.0 | °C | ASTM D746 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | > 1.0E+16 | ohms·cm | ASTM D257 |
| Dielectric Strength | > 22 | kV/mm | ASTM D149 |
| Dielectric Constant (23°C, 60 Hz) | 3.70 | ASTM D150 | |
| Dissipation Factor (23°C, 60 Hz) | 0.010 | ASTM D150 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index | 25 | % | ASTM D2863 |
| Radiant Panel Flame Spread Index | |||
| Flame test 2 | Pass | Multiple standards |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 55.0 | °C | |
| Drying Time | 2.0 - 8.0 | hr | |
| Cylinder Zone 1 Temp. | 96.0 | °C | |
| Melt Temperature | < 125 | °C |
| Extrusion instructions |
|---|
| Barrel 6: 110°C |
| Note Message | |
|---|---|
| 1 . | Compound, 23°C |
| 2 . | 20 AWG - 16 mil cable, ISO 6722/SAE J1128 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Developmental DTF1602.00 ESU | Trinseo | TPO | Developmental |
| Advanced-PP 1102L | Advanced Petrochemical Company | PP Homopolymer | Advanced-PP |
| ALTECH® PA6 A 1000/518 IM | ALBIS PLASTIC GmbH | Nylon 6 | ALTECH® PA6 |
| KEP® KEPA 1150 | Kumho Polychem Co., Ltd. | EPDM | KEP® |
| OXNILON 6 43GF | Oxford Polymers | Nylon 6 | OXNILON 6 |