Jampilen RP128M is a low sealing temperature polypropylene. The product is designed for coextruded bioriented polypropylene film and is formulated with a slip and antiblocking package. Jampilen RP128M exhibits very high transparency, excellent gloss and outstanding heat weldability. Films made with this grade show good hot tack and low seal initiation temperature (110 to 115°C). Due to its good flow properties, Jampilen RP128M can be coextruded with polypropylene grades with a relatively high melt flow rate. Coextruded BOPP films combine high resistance to moisture, fats, and oils, with good mechanical and optical properties. Jampilen RP128M is suitable for food contact.
General Information
Additive
  • Antiblock
  • Slip
Features
  • Antiblocking
  • Food Contact Acceptable
  • Good Flow
  • High Clarity
  • High Gloss
  • Hot Tack Strength
  • Low Temperature Heat Sealability
  • Moisture Resistant
  • Oil Resistant
  • Opticals
  • Slip
  • Terpolymer
  • Weldable
Uses
  • Bi-axially Oriented Film
  • Cosmetic Packaging
  • Film
  • Food Packaging
  • Shrink Wrap
  • Thin-walled Packaging
Processing Method
  • Bi-axially Oriented Film
  • Coextruded Film
  • Film Extrusion
PhysicalNominal ValueUnitTest Method
Density 0.900g/cm³ASTM D1505
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)8.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Rockwell Hardness (R-Scale)86ASTM D785
MechanicalNominal ValueUnitTest Method
Tensile Strength (Yield)22.0MPaASTM D638
Tensile Elongation (Yield)12%ASTM D638
Flexural Modulus 750MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (23°C)80J/mASTM D256
ThermalNominal ValueUnitTest Method
Deflection Temperature Under Load (0.45 MPa, Unannealed)65.0°CASTM D648
Vicat Softening Temperature 116°CASTM D1525 1
Accelerated Oven Ageing (150°C)360hrASTM D3012
OpticalNominal ValueUnitTest Method
Gloss 85ASTM D2457
Haze 1.8%ASTM D1003
Note Message
1 .Loading 1 (10 N)
Resin Grade Manufacturer Category Trademark
POWERSIL® XLR® 620 A/B Wacker Chemie AG Silicone POWERSIL®
S&E Wire & Cable GPE2001E-ROHS S&E Specialty Polymers, LLC PE, Unspecified S&E Wire & Cable
Vital-Line SHM3600 Teknor Apex Asia Pacific PTE. LTD. PVC, Flexible Vital-Line
ELASTOSIL® N 198 Wacker Chemie AG Silicone ELASTOSIL® N
ALTECH® PP-H B 4920/500 MR20 ALBIS PLASTIC GmbH PP Homopolymer ALTECH® PP-H