Category: | Nylon 11 , Polyamide 11 |
Manufacturer: | Arkema |
Trademark: | Rilsan® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | z65yYE_Rilsan-MB-3000.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Rilsan® MB 3000 is a Polyamide 11 (Nylon 11) product filled with filler. It can be processed by injection molding and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1080 | 1080 | kg/m³ | ISO 1183 1 |
Melt volume-flow rate (235°C/2.16 kg) | 95.0 | -- | cm³/10min | ISO 1133 2 |
Water Absorption | ISO 62 3 | |||
Saturation | 2.0 | -- | % | |
Equilibrium | 0.60 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile modulus | 2070 | 1920 | MPa | ISO 527-2 4 |
Tensile Stress (Yield) | 51.0 | 48.0 | MPa | ISO 527-2 5 |
Tensile Strain (Yield) | 5.0 | 5.0 | % | ISO 527-2 6 |
Nominal strain at break | > 50 | > 50 | % | ISO 527-2 7 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy notched impact strength | ISO 179/1eA 8 | |||
-30°C | 4.00 | 5.00 | kJ/m² | |
23°C | 4.00 | 5.00 | kJ/m² | |
Charpy impact strength | ISO 179/1eU 9 | |||
-30°C | 8.50 | -- | kJ/m² | |
23°C | -- | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Melting Temperature 10 | 189 | -- | °C | ISO 11357-3 11 |
CLTE - Flow | 1.0E-4 | -- | cm/cm/°C | ISO 11359-2 12 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface resistivity | -- | > 1.0E+15 | ohms | IEC 60093 13 |
Volume resistivity | > 1.0E+13 | > 1.0E+13 | ohms·m | IEC 60093 14 |
Electric strength | 28 | 28 | kV/mm | IEC 60243-1 15 |
Relative Permittivity | IEC 60250 16 | |||
100 Hz | 3.00 | -- | ||
1 MHz | 3.00 | -- | ||
Dissipation Factor | IEC 60250 17 | |||
100 Hz | 0.022 | -- | ||
1 MHz | 0.018 | -- | ||
Comparative tracking index | -- | 600 | IEC 60112 18 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | V-0 | -- | ISO 1210 19 | |
Burning Behav. at thickness h (0.800 mm) | V-0 | -- | ISO 1210 20 | |
Oxygen index | 33 | -- | % | ISO 4589-2 21 |
Note Message | |
---|---|
1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
10 . | 10 °C/min |
11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
14 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
16 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
17 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
18 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
19 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
20 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
21 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
VITAMIDE® BF13N2441/2 | Jackdaw Polymers | Nylon 6 | VITAMIDE® |
DOWLEX™ 2027G | The Dow Chemical Company | LMDPE | DOWLEX™ |
DOWLEX™ 2042G | The Dow Chemical Company | LLDPE | DOWLEX™ |
Electrafil® HDPE C BK | Techmer Engineered Solutions | HDPE | Electrafil® |
Kazan HDPE 293-284 | Kazanorgsintez Joint Stock Company | HDPE | Kazan HDPE |