20% GLASS BEADS REINFORCED POLYPROPYLENE COPOLYMER FOR INJECTION MOULDING APPLICATIONS.
General Information
Filler / Reinforcement
  • Glass beads, 20% filler by weight
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.990g/cm³ASTM D792, ISO 1183
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)11g/10 minASTM D1238, ISO 1133
MechanicalNominal ValueUnitTest Method
Tensile Modulus 1320MPaASTM D638, ISO 527-2
Tensile Strength (Yield)18.0MPaASTM D638, ISO 527-2
Tensile Elongation (Break)100%ASTM D638, ISO 527-2
Flexural Modulus 1030MPaASTM D790, ISO 178
Flexural Strength 25.0MPaASTM D790, ISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact
    23°C 65J/mASTM D256
    23°C 6.0kJ/m²ISO 180
ThermalNominal ValueUnitTest Method
Melting Temperature
    -- 167°CISO 11357-3
    -- 168°CASTM D3418
FlammabilityNominal ValueTest Method
Flame Rating (3.00 mm)HBUL 94
InjectionNominal ValueUnit
Rear Temperature 190 - 220°C
Middle Temperature 200 - 225°C
Front Temperature 205 - 230°C
Mold Temperature 30.0 - 65.0°C
Injection Pressure 70.0 - 105MPa
Holding Pressure 35.0 - 70.0MPa
Back Pressure 0.350 - 0.700MPa
Screw Speed 60 - 90rpm
Injection instructions
Fill Speed: 25 to 50 mm/sec
Resin Grade Manufacturer Category Trademark
VITAMIDE® BR3XNT6509 Jackdaw Polymers Nylon 6 VITAMIDE®
Nipol® DN202 Zeon Chemicals L.P. NBR Nipol®
EcoBlend® HCL7120 Shanghai KumhoSunny Plastics Co., Ltd. PLA+PMMA EcoBlend®
Kepex® 3330GK Korea Engineering Plastics Co., Ltd PBT Kepex®
HOPELEN SJ-170 Lotte Chemical Corporation PP Homopolymer HOPELEN