| Category: | SMA , Styrene Maleic Anhydride |
| Manufacturer: | Polyscope Polymers BV |
| Trademark: | XIRAN® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | yKHAPp_XIRAN-SZ23110.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
XIRAN® SZ23110 is an amorphous thermoplastic random SMA (styrene maleic anhydride) copolymer. XIRAN® SZ23110 is typically added to other engineering plastics to increase:
Application areas XIRAN® SZ23110 is specifically designed to be used in automotive interior application in combination with impact modifier (ABS) and optional glass fiber reinforcement. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.15 | g/cm³ | ISO 1183 |
| Apparent Density | 0.60 | g/cm³ | Internal method |
| Maleic Anhydride Content | 23 | % | Internal method |
| Molecular Weight | 110000 | g/mol | Internal method |
| Moisture Content | ppm | ISO 760 |
| Additional Information | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Pellet Size | 4.00 | mm | |
| Polydispersity - (Mw/Mn) | 2.50 | ISO 13885-1 | |
| Volatiles | ppm | GC |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glass Transition Temperature | 150 | °C | ISO 3146 |
| Vicat Softening Temperature | 145 | °C | ISO 306 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 - 90.0 | °C | |
| Drying Time | 2.0 - 3.0 | hr | |
| Rear Temperature | 230 - 250 | °C | |
| Middle Temperature | 230 - 250 | °C | |
| Front Temperature | 230 - 250 | °C | |
| Processing (Melt) Temp | < 280 | °C |
| Injection instructions |
|---|
| Optimum processing temperature: 240-270°C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 - 90.0 | °C | |
| Drying Time | 2.0 - 3.0 | hr | |
| Cylinder Zone 1 Temp. | 230 - 250 | °C | |
| Cylinder Zone 2 Temp. | 230 - 250 | °C | |
| Cylinder Zone 3 Temp. | 230 - 250 | °C | |
| Cylinder Zone 4 Temp. | 230 - 250 | °C | |
| Cylinder Zone 5 Temp. | 230 - 250 | °C |
| Extrusion instructions |
|---|
| Optimum processing temperature: 240-270°CMaximum processing temperature: 280°C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TOPAS® Elastomer E-140 | Topas Advanced Polymers, Inc. | COC | TOPAS® |
| Titalon® 3400GF | Titan Plastics Compounds Co., Ltd. | Nylon 12 | Titalon® |
| EnCom PC1613 | EnCom, Inc. | PC | EnCom |
| Shida 2520A | JINJIANG City SHIDA Plastic Fine Co., Ltd. | TPE | Shida |
| LEXAN™ 923A resin | SABIC Innovative Plastics | PC | LEXAN™ |