Category: | ABS , Acrylonitrile Butadiene Styrene |
Manufacturer: | TER HELL PLASTIC GMBH |
Trademark: | TEREZ ABS |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | y3IOQU_TEREZ-ABS-3003.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
High impact ABS. For moulding parts with high impact resistance. |
General Information | |
---|---|
Features |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.03 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 6.0 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 1900 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 40.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 3.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-30°C | 13 | kJ/m² | |
23°C | 35 | kJ/m² | |
Charpy Unnotched Impact Strength (23°C) | No Break | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, Unannealed | 89.0 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 76.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | 90.0 | °C | ISO 306/B50 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Comparative Tracking Index | 600 | V | IEC 60112 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
VYLOPET® EMC310TU | TOYOBO America, Inc. | PC+PBT | VYLOPET® |
Crastin® FG6129 NC010 | DuPont Performance Polymers | PBT | Crastin® |
Grivory® HT3Z black 9564 | EMS-GRIVORY | Nylon 10T/X | Grivory® |
Karina MBPP WHITE 1100/2350-IE | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
Lupolen 5261 Z Q 456 | LyondellBasell Industries | HDPE | Lupolen |