LNP THERMOCOMP AB002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Bead. Also known as: LNP* THERMOCOMP* Compound AB-1002 Product reorder name: AB002 |
General Information | |
---|---|
Filler / Reinforcement |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.12 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (24 hr) | 0.70 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus 1 | 2570 | MPa | ASTM D638 |
Tensile Strength (Break) | 34.5 | MPa | ASTM D638 |
Tensile Elongation (Break) | 3.1 | % | ASTM D638 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 110 | J/m | ASTM D256 |
Unnotched Izod Impact (23°C) | 660 | J/m | ASTM D4812 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 82.2 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.050 - 0.10 | % | |
Rear Temperature | 204 - 216 | °C | |
Middle Temperature | 232 - 243 | °C | |
Front Temperature | 266 - 277 | °C | |
Processing (Melt) Temp | 260 | °C | |
Mold Temperature | 71.1 - 82.2 | °C | |
Back Pressure | 0.172 - 0.344 | MPa | |
Screw Speed | 30 - 60 | rpm |
Note Message | |
---|---|
1 . | 50 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Riblene® FH 39 F | Versalis S.p.A. | LDPE | Riblene® |
Sarlink® TPV 2540DN | Teknor Apex Company | TPV | Sarlink® TPV |
Tecodur® PB70 NL IM | Eurotec Engineering Plastics | PBT | Tecodur® |
Edistir® RT 461F | Versalis S.p.A. | PS (HIPS) | Edistir® |
Idemitsu PS SEHI-107 | Idemitsu PS | PS (HIPS) | Idemitsu PS |