Staramide PF005

Category: Nylon 6 , Polyamide 6
Manufacturer: Eurostar Engineering Plastics
Trademark: Staramide
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: xKn7fe_Staramide-PF005.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Staramide PF005 is a 25 % Glass Fiber Reinforced Polyamide 6 Injection Molding Resin
General Information
Filler / Reinforcement
  • Glass Fiber, 25% Filler by Weight
RoHS Compliance
  • RoHS Compliant
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Density 1.31g/cm³ISO 1183
Molding Shrinkage - Flow 10.20 to 0.40%Internal Method
Water Absorption (Saturation, 23°C)6.5%ISO 62
MechanicalNominal ValueUnitTest Method
Tensile Stress (Break)145MPaISO 527-2/5
Tensile Strain (Break)3.0%ISO 527-2/5
Flexural Modulus 27500MPaISO 178
Flexural Stress 190MPaISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength 3(23°C)10kJ/m²ISO 180/1A
Unnotched Izod Impact Strength 4(23°C)50kJ/m²ISO 180/1U
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature 5
    0.45 MPa, Unannealed, 100 mm Span 215°CISO 75-2/Be
    1.8 MPa, Unannealed, 100 mm Span 205°CISO 75-2/Ae
Ball Pressure Test 6(125°C)PassIEC 60695-10-2
InjectionNominal ValueUnit
Drying Temperature 75.0 to 85.0°C
Drying Time 4.0 to 6.0hr
Suggested Max Moisture 0.20%
Rear Temperature 230 to 240°C
Middle Temperature 240 to 250°C
Front Temperature 240 to 270°C
Processing (Melt) Temp 240 to 270°C
Mold Temperature 60.0 to 80.0°C
Note Message
1 .Tensile Bar
2 .2.0 mm/min
3 .80*10*4
4 .80*10*4
5 .120*10*4
6 .125 ±2°C
Resin Grade Manufacturer Category Trademark
SEPTON™ 2063 Kuraray Co., Ltd. SEPS SEPTON™
Smooth-On Psycho Paint® Smooth-On, Inc Silicone Smooth-On
OXNILON 6 15IMP Oxford Polymers Nylon 6 OXNILON 6
LUVOCOM® 1100-8549 LEHVOSS Group PESU LUVOCOM®
LEXAN™ LUX9612G resin SABIC Innovative Plastics Europe PC LEXAN™