Category: | PUR-Ether/MDI , Polyurethane (Polyether, MDI) |
Manufacturer: | Chemtura |
Trademark: | Vibrathane® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | xHOH0s_Vibrathane-B875.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
VIBRATHANE B875 is an MDI-terminated, polyether based prepolymer. The prepolymer is a liquid at room temperature. VIBRATHANE B875 yields a 95 Shore hardness urethane when cured with 1,4 Butanediol. |
General Information | |
---|---|
Forms |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
Durometer Hardness (Shore A) | 95 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Compressive Strength | ASTM D695 | ||
5% Strain | 1.90 | MPa | |
10% Strain | 3.43 | MPa | |
15% Strain | 5.05 | MPa | |
20% Strain | 7.15 | MPa | |
25% Strain | 9.88 | MPa |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% Strain | 8.69 | MPa | |
200% Strain | 10.3 | MPa | |
300% Strain | 11.8 | MPa | |
Tensile Strength | 16.5 | MPa | ASTM D412 |
Tensile Elongation (Break) | 480 | % | ASTM D412 |
Tear Strength | |||
-- 1 | 78.8 | kN/m | ASTM D624 |
Split | 20 | kN/m | ASTM D470 |
Compression Set (80°C, 22 hr) | 30 | % | ASTM D395 |
Bayshore Resilience | 50 | % | ASTM D2632 |
Thermoset | Nominal Value | Unit | |
---|---|---|---|
Pot Life | 5.0 | min | |
Post Cure Time (115°C) | 4.0 | hr |
Uncured Properties | Nominal Value | Unit | |
---|---|---|---|
Curing Time (82°C) | 1.0 | hr |
Note Message | |
---|---|
1 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 1381 P-1 TFE 20 | RTP Company | PPS | RTP |
NAXELL™ PC23M-10G | MRC Polymers, Inc. | PC | NAXELL™ |
DENIBLEND A | Vamp Tech | PC+ABS | DENIBLEND |
Jam PE 20516 | Jam Petrochemical Company | LLDPE | Jam PE |
Karina BLACK PVC COMPOUND 880-48/ 1-E-IS-LMP | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |