Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® A |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | wlVmGB_TECHNYL-A-218-V35-BLACK-34-NG.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Processing Method |
|
Part Marking Code (ISO 11469) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.41 | -- | g/cm³ | ISO 1183/A |
Water Absorption (23°C, 24 hr) | 0.75 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 12000 | 8700 | MPa | ISO 527-2/1A |
Tensile Stress (Break) | 210 | 150 | MPa | ISO 527-2/1A |
Tensile Strain (Break) | 3.0 | 4.0 | % | ISO 527-2/1A |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 14 | 19 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 95 | 100 | kJ/m² | ISO 179/1eU |
Notched Izod Impact Strength (23°C) | 13 | 18 | kJ/m² | ISO 180/1A |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 255 | -- | °C | ISO 75-2/Af |
Melting Temperature | 260 | -- | °C | ISO 11357-3 |
CLTE - Flow (23 to 85°C) | 2.2E-5 | -- | cm/cm/°C | ISO 11359-2 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 6.0E+14 | 1.0E+12 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
Electric Strength | 34 | 29 | kV/mm | IEC 60243-1 |
Dissipation Factor | 0.010 | 0.11 | IEC 60250 | |
Comparative Tracking Index (Solution A) | 600 | 600 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (0.800 mm) | HB | -- | UL 94 | |
Oxygen Index | 23 | -- | % | ISO 4589-2 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 260 to 270 | °C | |
Middle Temperature | 270 to 280 | °C | |
Front Temperature | 280 to 290 | °C | |
Mold Temperature | 70.0 to 100 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Santoprene™ 8281-75MED | ExxonMobil Chemical | TPV | Santoprene™ |
TRANSMARE® 14CNF30-0.001 | Transmare Compounding B.V. | PP Copolymer | TRANSMARE® |
Ultramid® T KR 4365 G5 | BASF Corporation | Nylon 6/6T | Ultramid® |
NOVALAST® 6001 | NOVA Polymers, Inc. | TPV | NOVALAST® |
LUBEMID B27 NATURAL UV | LUBEN PLAST srl | Nylon 6 | LUBEMID |