Luranyl® HT 240 G4

Category: PPE+Nylon 66 , Polyphenylene Ether + Nylon 66
Manufacturer: ROMIRA GmbH
Trademark: Luranyl®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: wgBlzF_Luranyl-HT-240-G4.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
PPE+PA Blend with 20% glass fibre; very high heat resistance
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 20% filler by weight
Features
  • Heat resistance, high
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 1.23g/cm³ISO 1183
Melt Volume-Flow Rate (MVR) (280°C/5.0 kg)50.0cm³/10minISO 1133
Water Absorption (23°C, 24 hr)< 0.37%ISO 62
MechanicalNominal ValueUnitTest Method
Tensile Modulus (23°C)6300MPaISO 527-2/1
Tensile Stress (Yield, 23°C)120MPaISO 527-2/50
Tensile Strain (Break, 23°C)7.0%ISO 527-2/50
ImpactNominal ValueUnitTest Method
Charpy Unnotched Impact Strength ISO 179/1eU
    -30°C 50kJ/m²ISO 179/1eU
    23°C 65kJ/m²ISO 179/1eU
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)210°CISO 75-2/A
Vicat Softening Temperature 240°CISO 306/B50
FlammabilityNominal ValueTest Method
Flame Rating (1.60 mm)HBUL 94
InjectionNominal ValueUnit
Drying Temperature 80.0 - 100°C
Drying Time 2.0 - 4.0hr
Suggested Max Moisture 0.050%
Processing (Melt) Temp 285 - 310°C
Mold Temperature 90.0 - 120°C
Injection Rate Moderate
Screw Speed 12 - 18rpm
Injection instructions
Maximum Residence Time: 4 to 10 minInjection Pressure: moderate to high
Resin Grade Manufacturer Category Trademark
Metabolix I6003rp Metabolix PHA Metabolix
ResMart Ultra HDPE 20 ResMart HDPE ResMart Ultra
Sylvin RP 3300 Natural Sylvin Technologies Incorporated PVC, Rigid Sylvin
ABS Proquigel AM-F Proquigel ABS ABS Proquigel
Edgetek™ CY1000-20CF/000 BK001 PolyOne Corporation PC+ABS Edgetek™