| Polypropylene %30 glass fiber reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.10 to 1.15 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 13 to 17 | g/10 min | ISO 1133 |
| Molding Shrinkage | 0.30 to 0.50 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 70 to 75 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 6000 to 10000 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 60.0 to 100 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 4.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | > 9.0 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 120 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 105 | °C | ISO 306/B |
| Melting Temperature (DSC) | 160 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Moplen HP461Y | PolyMirae | PP, Unspecified | Moplen |
| Varcum 29607 | Durez Corporation | Phenolic | Varcum |
| Zytel® HTN 52G35EF BK420 | DuPont Performance Polymers | PPA | Zytel® HTN |
| ACRYLITE® Film White WF003 | Evonik Cyro LLC | Film, PMMA | ACRYLITE® Film |
| Algoflon® F 7 | Solvay Specialty Polymers | PTFE | Algoflon® |