| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Teknor Apex Company (Chem Polymer) |
| Trademark: | Chemlon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | w7M2aW_Chemlon-115-GH.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Chemlon® 115 GH is a Polyamide 66 (Nylon 66) material filled with 15% glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Important attributes of Chemlon® 115 GH are:
|
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.24 | g/cm³ | ASTM D792 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 110 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 2.0 | % | ASTM D638 |
| Flexural Modulus | 5170 | MPa | ASTM D790 |
| Flexural Strength | 176 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 64 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | 243 | °C | ASTM D648 |
| Melting Temperature | 254 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Polytron® P50N07 | Polyram Ram-On Industries | PP, Unspecified | Polytron® |
| STRANOX H-PP50%LFT | Oxford Polymers | PP Homopolymer | STRANOX |
| Durethan® DP 1441/40 H3.0 EF 000000 | LANXESS Corporation | Nylon 6 | Durethan® |
| SIBUR Synthetic Rubber DST-30R-01 Group 1 | SIBUR | SBC | SIBUR Synthetic Rubber |
| TAFMER™ H-5030S | Mitsui Chemicals, Inc. | PAO | TAFMER™ |