| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | Teknor Apex Company |
| Trademark: | Monprene® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | vrs7zw_Monprene-MP-3955B.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Monprene®MP-3955B is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Typical application areas include:
|
| General Information | |
|---|---|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.18 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (200°C/5.0 kg) | 32 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 81 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 10.0 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 650 | % | ASTM D412 |
| Tear Strength | 38.5 | kN/m | ASTM D624 |
| Compression Set | ASTM D395 | ||
| 23°C, 22 hr | 35 | % | ASTM D395 |
| 70°C, 22 hr | 57 | % | ASTM D395 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | -60.0 | °C | ASTM D746 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 182 - 232 | °C | |
| Middle Temperature | 188 - 238 | °C | |
| Front Temperature | 193 - 243 | °C | |
| Nozzle Temperature | 199 - 249 | °C | |
| Processing (Melt) Temp | 199 - 249 | °C | |
| Mold Temperature | 35.0 - 48.9 | °C | |
| Injection Pressure | 1.38 - 5.52 | MPa | |
| Injection Rate | Fast | ||
| Back Pressure | 0.172 - 0.689 | MPa | |
| Screw Speed | 50 - 100 | rpm | |
| Cushion | 3.81 - 25.4 | mm |
| Injection instructions |
|---|
| Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C). |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 182 - 232 | °C | |
| Cylinder Zone 2 Temp. | 188 - 238 | °C | |
| Cylinder Zone 3 Temp. | 193 - 243 | °C | |
| Cylinder Zone 5 Temp. | 199 - 249 | °C | |
| Die Temperature | 199 - 249 | °C |
| Extrusion instructions |
|---|
| Screw Speed: 30 to 100 rpm |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sylvin 8948-70 Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| Axiall PVC 4125-52 | Axiall Corporation | PVC, Flexible | Axiall PVC |
| Lotrène® LLDPE Q1018N | QATOFIN Company Limited | LLDPE | Lotrène® LLDPE |
| POTICON BT212N | Otsuka Chemical Co., Ltd. | PBT | POTICON |
| XENOY™ X5230 resin | SABIC Innovative Plastics Europe | PC+PET | XENOY™ |