Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
Manufacturer: | SO.F.TER. SPA |
Trademark: | Laprene® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | v84IA5_Laprene-830000969.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Laprene® 830000969 is a Styrene Ethylene Butylene Styrene Block Copolymer (SEBS) material. It is available in Europe, Latin America, or North America for injection molding. Primary attribute of Laprene® 830000969: REACH Compliant. Typical applications include:
|
General Information | |
---|---|
Uses |
|
Agency Ratings |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.890 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 3 sec) | 67 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Set | 6 | % | ASTM D412 |
Tensile Stress 1(100% Strain) | 1.80 | MPa | ASTM D412 |
Tensile Strength 2 | 12.0 | MPa | ASTM D412 |
Tensile Elongation 3(Break) | 790 | % | ASTM D412 |
Tear Strength 4 | 33.0 | kN/m | ASTM D624 |
Compression Set 5(70°C, 22 hr) | 44 | % | ASTM D395B |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 170 | °C | |
Middle Temperature | 180 | °C | |
Front Temperature | 180 | °C | |
Nozzle Temperature | 190 | °C | |
Mold Temperature | 20.0 to 40.0 | °C |
Note Message | |
---|---|
1 . | Die C |
2 . | Die C |
3 . | Die C |
4 . | Die C |
5 . | Type 1 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sylvin 6198-85 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Versalloy™ HC 9220-70 | PolyOne Corporation | TPE | Versalloy™ |
ULTZEX™ 4570 | Prime Polymer Co., Ltd. | LLDPE | ULTZEX™ |
APEX® 96-A0097D-85 | Teknor Apex Company | PVC, Flexible | APEX® |
TechnoFin PP T 22 | TechnoCompound GmbH | PP, Unspecified | TechnoFin |