TECHNYL® A 216 V20 BLACK 21N

Category: Nylon 66 , Polyamide 66
Manufacturer: Solvay Engineering Plastics
Trademark: TECHNYL®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: umwVR6_TECHNYLA216V20BLACK21N.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
TECHNYL® A 216 V20 Black 21N is a polyamide 66, reinforced with 20% of glass fibre, for injection moulding. This grade offers an excellent combination between thermal and mechanical properties.
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 20% filler by weight
Features
  • Good dimensional stability
  • Good liquidity
  • Good demoulding performance
Uses
  • Electrical/Electronic Applications
Agency Ratings
  • EC 1907/2006 (REACH)
  • UL QMFZ2
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
  • Grey
  • Blue
  • Natural color
Forms
  • Particle
Processing Method
  • Injection molding
Multi-Point Data
  • Isothermal Stress vs. Strain (ISO 11403-1)
Resin ID (ISO 1043)
  • PA66-GF20
PhysicalDryConditionedUnitTest Method
Density 1.28--g/cm³ISO 1183/A
Water Absorption ISO 62
     23°C, 24 hr 1.0--%ISO 62
     Saturated, 23°C 6.6--%ISO 62
     Equilibrium, 23°C, 50% RH 2.5--%ISO 62
MechanicalDryConditionedUnitTest Method
Tensile Modulus (23°C)74005000MPaISO 527-2/1A
Tensile Stress (Break, 23°C)145100MPaISO 527-2/1A
Tensile Strain (Break, 23°C)3.015%ISO 527-2
Flexural Modulus (23°C)68004500MPaISO 178
Flexural Stress (23°C)225150MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength (23°C)7.09.0kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength
     23°C 5080kJ/m²ISO 179/1eU
     23°C 40--kJ/m²ISO 179/1fU
Notched Izod Impact (23°C)7.09.0kJ/m²ISO 180
Unnotched Izod Impact Strength (23°C)4565kJ/m²ISO 180/1U
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)245--°CISO 75-2/Af
Melting Temperature 262--°CISO 11357-3
ElectricalDryConditionedUnitTest Method
Surface Resistivity 6.0E+151.0E+13ohmsIEC 60093
Volume Resistivity 1.0E+152.0E+15ohms·cmIEC 60093
Dielectric Strength (2.00 mm)3228kV/mmIEC 60243-1
Relative Permittivity 3.704.00IEC 60250
Dissipation Factor 0.0100.11IEC 60250
Comparative Tracking Index IEC 60112
     Solution a 600600VIEC 60112
     Solution B 525525VIEC 60112
FlammabilityDryConditionedUnitTest Method
Flame Rating (1.6 mm)HB--UL 94
Glow Wire Flammability Index (1.6 mm)650--°CIEC 60695-2-12
Oxygen Index 23--%ISO 4589-2
InjectionDryUnit
Drying Temperature 80°C
Suggested Max Moisture 0.20%
Rear Temperature 270 - 280°C
Middle Temperature 275 - 285°C
Front Temperature 280 - 290°C
Mold Temperature 70 - 100°C
Injection instructions
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design
Resin Grade Manufacturer Category Trademark
RTP 1303 TFE 20 RTP Company PPS RTP
Niuk 50GP30 Shanghai Niuk New Plastic Technology Co., Ltd. Nylon 66 Niuk
Braskem PE GP5550BX Braskem HDPE Braskem PE
Elastron® G G400.A65.B Elastron USA, Inc. SEBS Elastron® G
Osterlene® PPH-12-.8 Osterman & Company PP Homopolymer Osterlene®