| Data was measured on natural colored test specimens. |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.13 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (3.18 mm) | 0.80 to 1.1 | % | ASTM D955 |
| Water Absorption (24 hr) | 1.6 | % | ASTM D570 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale) | 120 | ASTM D785 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 82.7 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 17 | % | ASTM D638 |
| Flexural Modulus | 3030 | MPa | ASTM D790 |
| Flexural Strength | 117 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (6.35 mm) | 48 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load | ASTM D648 | ||
| 0.45 MPa, Unannealed | 185 | °C | |
| 1.8 MPa, Unannealed | 71.1 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| THERMOLAST® K TP7HPN (Series: EX/UV) | KRAIBURG TPE | TPE | THERMOLAST® K |
| NANTEX® 257AX4 | Nantex Industry Co., Ltd. | SBR, Unspecified | NANTEX® |
| 4MID® 9AB23500 | 4Plas | Nylon 66/6 | 4MID® |
| Hax™ HFX 507 | Fainplast Compounds S.r.l | Polyolefin, Unspecified | Hax™ |
| OXNILON 6 15IMP | Oxford Polymers | Nylon 6 | OXNILON 6 |