Andur 70 DP/Curene® 442

Category: PUR-Ether/TDI , Polyurethane (Polyether, TDI)
Manufacturer: Anderson Development Company
Trademark: Andur
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: uFGLzD_Andur-70-DP-Curene-442.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Andur 70-DP is a polyether (PTMG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 70 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, or by the use of plasticizers.
General Information
Forms
  • Liquid
PhysicalNominal ValueUnitTest Method
Density 1.18g/cm³ASTM D1505
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D)71ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress (100% Strain)29.2MPaASTM D412
Tensile Strength (Yield)57.2MPaASTM D412
Tensile Elongation (Break)83%ASTM D412
Compression Set 33%ASTM D395B
Bayshore Resilience 45%ASTM D2632
ThermosetNominal ValueUnit
Pot Life 1.0 - 1.5min
Demold Time (100°C)15min
Post Cure Time (100°C)16hr
Additional Information
Durometer Hardness, ASTM D2240, Shore D: 68 to 73Die C Tear, ASTM D1004: 976 pliAverage Split Tear, ASTM D1938: 319 pliStoichiometry Curative Level: 95%Mix Temperature: Andur 70-DP: 180-212°F Curene 442: 250°F
Resin Grade Manufacturer Category Trademark
ASTALOY™ MB2106 Marplex Australia Pty. Ltd. PC ASTALOY™
Chemlon® 60AIM Teknor Apex Company (Chem Polymer) Nylon 6 Chemlon®
HiFill® PA6 IM 511 HS L Techmer Engineered Solutions Nylon 6 HiFill®
LNP™ VERTON™ RV008E compound SABIC Innovative Plastics Nylon 66 LNP™ VERTON™
Orevac® 18751 Arkema PP Homopolymer Orevac®