30% Glass Reinforced Polyethylene Terephthalate Developed for Food Contact Applications |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Forms |
|
Processing Method |
|
Part Marking Code (ISO 11469) |
|
Resin ID (ISO 1043) |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.57 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.80 | % | |
Flow | 0.20 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 10500 | MPa | ISO 527-2 |
Tensile Stress (Break) | 162 | MPa | ISO 527-2 |
Tensile Strain (Break) | 2.1 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 11 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 40 | kJ/m² | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 242 | °C | ISO 75-2/A |
Melting Temperature 1 | 257 | °C | ISO 11357-3 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Comparative Tracking Index | 250 | V | IEC 60112 |
Note Message | |
---|---|
1 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Small Boss STPR005 | Tongxiang Small Boss Special Plastic Products Co., Ltd. | SBS | Small Boss |
GAPEX® RPP20DA03NA | Ferro Corporation | PP Homopolymer | GAPEX® |
INEOS PP 240-CA12 | INEOS Olefins & Polymers Europe | PP Random Copolymer | INEOS PP |
ISOTHANE® G1680A-E | Great Eastern Resins Industrial Co Ltd (GRECO) | TPU-Polyether | ISOTHANE® |
Plaslube® PA6/6 CF30 TS12 BK | Techmer Engineered Solutions | Nylon 66 | Plaslube® |