| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | UNITIKA Plastics Division |
| Trademark: | UNITIKA Nylon 6 |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | tcOZ0m_UNITIKA-Nylon-6-M1030DH.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Nano composite nylon |
| General Information | |
|---|---|
| Uses |
|
| Forms |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.15 | 1.15 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | |||
| Across Flow : 3.20 mm | 1.0 | 1.0 | % | |
| Flow : 3.20 mm | 0.80 | 0.80 | % | |
| Water Absorption | ISO 62 | |||
| 23°C, 24 hr | 0.90 | 0.90 | % | |
| Equilibrium, 23°C, 50% RH | 2.8 | 2.8 | % |
| Hardness | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Rockwell Hardness (R-Scale) | 114 | -- | ISO 2039-2 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 4300 | 2600 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 95.0 | 63.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 3.4 | 4.0 | % | ISO 527-2 |
| Flexural Modulus | 4500 | 2500 | MPa | ISO 178 |
| Flexural Stress | 155 | 66.0 | MPa | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 4.0 | 7.0 | kJ/m² | ISO 179 |
| Charpy Unnotched Impact Strength | 57 | 70 | kJ/m² | ISO 179 |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature | ||||
| 0.45 MPa, Unannealed | 186 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 140 | -- | °C | ISO 75-2/A |
| CLTE - Flow | 5.3E-5 | 5.3E-5 | cm/cm/°C | ISO 11359-2 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Volume Resistivity | 1.0E+15 | -- | ohms·cm | IEC 60093 |
| Electric Strength (1.00 mm) | 42 | -- | kV/mm | IEC 60243-1 |
| Dielectric Constant (1 MHz) | 3.70 | -- | IEC 60250 | |
| Dissipation Factor (1 MHz) | 0.019 | -- | IEC 60250 | |
| Comparative Tracking Index | 475 | 475 | V | IEC 60112 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Romiloy® 1035 F | ROMIRA GmbH | PC+ABS | Romiloy® |
| Sindustris PC EC5001AF | Sincerity Australia Pty Ltd. | PC | Sindustris PC |
| Topilene® J945 | Hyosung Corporation | PP Impact Copolymer | Topilene® |
| VITAMIDE® BR36BK9006 | Jackdaw Polymers | Nylon 6 | VITAMIDE® |
| Vital-Line SHM2507G | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | Vital-Line |