Category: | ABS , Acrylonitrile Butadiene Styrene |
Manufacturer: | TER HELL PLASTIC GMBH |
Trademark: | TEREZ ABS |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | tZVTRE_TEREZ-ABS-3320-A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Antistatic ABS with high gloss and good impact strength. For long moulding parts of all kind with high flow facilities. |
General Information | |
---|---|
Additive |
|
Features |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.04 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 34 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2300 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 44.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 2.4 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 19 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 130 | kJ/m² | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, Unannealed | 95.0 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 99.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | 95.0 | °C | ISO 306/B50 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Comparative Tracking Index | 600 | V | IEC 60112 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Silamid® SV35 | Roonamid a.s. | Nylon 6 | Silamid® |
SUPREME Specialty PS SP6409 | Supreme Petrochem Ltd. | PS (Specialty) | SUPREME Specialty PS |
Cevian®-S CSS200-10 | PlastxWorld Inc. | PC Alloy | Cevian®-S |
Dryflex® 600550S | ELASTO | SEBS | Dryflex® |
Panlite® BN-8110R | TEIJIN LIMITED | PC | Panlite® |