| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | BASF Corp. Thermoplastic Polyurethanes |
| Trademark: | Elastollan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | tXR41P_Elastollan-S60DN.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Elastollan® S60DN exhibits excellent abrasion resistance, toughness, good heat, oil, fuel, and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® S60DN is supplied uncolored in diced form. |
| General Information | |
|---|---|
| Features |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.25 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 60 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus (Injection Molded) | 186 | MPa | ASTM D412 |
| Flexural Modulus (Injection Molded) | 152 | MPa | ASTM D790 |
| Taber Abrasion Resistance | 50.0 | mg | ASTM D1044 |
| Abrasion - DIN | 25 | mm³ | DIN 53516 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Softening Point - DMA | 147 | °C | Internal Method |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% Strain | 22.1 | MPa | |
| 300% Strain | 44.8 | MPa | |
| Tensile Strength | 50.3 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 400 | % | ASTM D412 |
| Tear Strength 1 | 228 | kN/m | ASTM D624 |
| Compression Set | ASTM D395B | ||
| 23°C, 22 hr | 40 | % | |
| 70°C, 22 hr | 50 | % |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glass Transition Temperature | -8.00 | °C | Internal Method |
| Vicat Softening Temperature | 145 | °C | ASTM D1525 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 110 to 120 | °C | |
| Drying Time | 2.0 to 3.0 | hr | |
| Suggested Max Moisture | 0.030 | % | |
| Rear Temperature | 210 to 230 | °C | |
| Middle Temperature | 210 to 230 | °C | |
| Front Temperature | 210 to 230 | °C | |
| Nozzle Temperature | 220 to 240 | °C |
| Note Message | |
|---|---|
| 1 . | Die C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxxam™ RB 135601 | PolyOne Corporation | TPO | Maxxam™ |
| RTP 1000 TFE 20 FR A | RTP Company | PBT | RTP |
| Shandong PA610 GYEHVN | Shandong Guangyin New Materials Co., Ltd. | Nylon 610 | Shandong PA610 |
| Staramide R1000 | Eurostar Engineering Plastics | Nylon 66 | Staramide |
| Thanelene® TPU S80A15 PRTA010 TP305 MSP | Petropol Industry and Trade of Polymers LTDA | TPU-Polyester | Thanelene® TPU |