| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Barnet |
| Trademark: | Envir® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | sxMQ3G_Envir-PA66T2HL-BK0603.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Envir® PA66T2HL-BK0603 is a highly Toughened Nylon 66 molding resin, it is Heat stabilized and Lubricated for high performance and processing. 66T2HL offers a versatile balance of strength and toughness, it is provided Black in color. |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Appearance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.11 | g/cm³ | ASTM D792 |
| Melt Volume-Flow Rate (MVR) (275°C/5.0 kg) | 30.0 | cm³/10min | ASTM D1238 |
| Moisture Content | < 0.20 | % | ASTM D6980 |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Granularity | 1.50 | g/100 pellets |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2580 | MPa | ISO 527-2 |
| Tensile Stress | ISO 527-2 | ||
| Yield | 60.0 | MPa | |
| Break | 50.0 | MPa | |
| Tensile Strain | ISO 527-2 | ||
| Yield | 4.3 | % | |
| Break | 28 | % | |
| Flexural Modulus | 2380 | MPa | ISO 178 |
| Flexural Stress | 92.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 18 | kJ/m² | ISO 180/A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Peak Melting Temperature | 260 | °C | ASTM D3418 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sylvin 5175-92 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| ADDINYL B2I V25 | ADDIPLAST | Nylon 6 | ADDINYL |
| LUBEMID B27 NATURAL UV | LUBEN PLAST srl | Nylon 6 | LUBEMID |
| Petrothene® NA345 | LyondellBasell Industries | LDPE | Petrothene® |
| KIBISAN® PN-127 L100 FG | CHI MEI CORPORATION | SAN | KIBISAN® |