TECHNYL® C 218 MZ20 V10 BLACK

Category: Nylon 6 , Polyamide 6
Manufacturer: Solvay Engineering Plastics
Trademark: TECHNYL®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: sxM2ge_TECHNYLC218MZ20V10BLACK.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
TECHNYL® C 218 MZ20 V10 Black is a polyamide 6, reinforced 20 % mineral filler and 10 % of glass fibre, heat stabilized, for injection moulding. This grade offers an excellent planarity of the end product, good mechanical properties and a high dimensional stability.
General Information
Filler / Reinforcement
  • Glass \mineral, 30% filler by weight
Additive
  • heat stabilizer
Features
  • Heat Stabilized - Inorganic
  • Good dimensional stability
  • Low warpage
  • Rigid, good
Uses
  • Application in Automobile Field
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Injection molding
Multi-Point Data
  • Isothermal Stress vs. Strain (ISO 11403-1)
Resin ID (ISO 1043)
  • PA6-MD20+GF10
PhysicalDryConditionedUnitTest Method
Density 1.36--g/cm³ISO 1183/A
MechanicalDryConditionedUnitTest Method
Tensile Modulus (23°C)74004500MPaISO 527-2/1A
Tensile Stress (Break, 23°C)10060.0MPaISO 527-2/1A
Tensile Strain (Break, 23°C)3.3--%ISO 527-2
Flexural Modulus (23°C)9300--MPaISO 178
Flexural Stress (23°C)255--MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength (23°C)1410kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength (23°C)6085kJ/m²ISO 179/1eU
Notched Izod Impact (23°C)15--kJ/m²ISO 180
Unnotched Izod Impact Strength (23°C)82--kJ/m²ISO 180/1U
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)205--°CISO 75-2/Af
Melting Temperature 222--°CISO 11357-3
InjectionDryUnit
Drying Temperature 80°C
Suggested Max Moisture 0.20%
Rear Temperature 230 - 235°C
Middle Temperature 235 - 240°C
Front Temperature 240 - 250°C
Mold Temperature 60 - 90°C
Injection instructions
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C.
Resin Grade Manufacturer Category Trademark
Andur 8-5 APLF Anderson Development Company PUR-Ester/TDI Andur
ASTALOY™ PC/ABS MDA216 Marplex Australia Pty. Ltd. PC+ABS ASTALOY™
HIDEN® F600 YUHWA Korea Petrochemical Ind. Co., Ltd. HDPE HIDEN®
Sylvin 6240-80 Yellow 4191 Sylvin Technologies Incorporated PVC, Unspecified Sylvin
Marlex® TRB-432 Chevron Phillips Chemical Company LLC HDPE Marlex®