Monprene® RG-17270 (PRELIMINARY DATA)

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Monprene®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: sP46vh_MonpreneRG17270PRELIMINARYDATA.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
The Monprene RG-17200 series is a group of high performance thermoplastic elastomers specifically designed with medium density for regulated applications including food contact, toys, and children's products. Monprene RG-17270 is a medium density, medium hardness grade that complies with various European regulations and directives for food contact and toy safety and is suitable for injection molding. Please contact Teknor Apex for a regulatory compliance letter.
General Information
Features
  • High elasticity
  • smoothness
  • Workability, good
  • Good coloring
  • Good adhesion
  • Medium liquidity
  • Lubrication
  • Compliance of Food Exposure
  • Fill
  • Medium density
  • Medium hardness
Uses
  • Cosmetic Packaging
  • Handle
  • Kitchen utensils
  • Washer
  • Non-specific food applications
  • Cover
  • Food packaging
  • Food service sector
  • Food container
  • Toys
  • Rubber substitution
  • Consumer goods application field
  • Toothbrush handle
Agency Ratings
  • FDA Food Exposure, Not Rated
  • European food contact, not rated
RoHS Compliance
  • RoHS compliance
Appearance
  • Opacity
  • Available colors
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 1.05g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)12g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness
    Shaw A, 1 sec 72ASTM D2240
    Shaw A, 5 seconds 70ISO 868
ElastomersNominal ValueUnitTest Method
Tensile Stress ISO 37
    100% strain 2.30MPaISO 37
    300% strain 2.40MPaISO 37
Tensile Strength (Break)8.30MPaISO 37
Tensile Elongation (Break)700%ISO 37
Compression Set 1ISO 815
    23°C, 22 hr 34%ISO 815
    70°C, 22 hr 55%ISO 815
Fill AnalysisNominal ValueUnitTest Method
Apparent Viscosity (200°C, 206 sec^-1)110Pa·sISO 11443
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Rear Temperature 120 - 160°C
Middle Temperature 160 - 230°C
Front Temperature 180 - 230°C
Nozzle Temperature 180 - 230°C
Processing (Melt) Temp 180 - 230°C
Mold Temperature 15 - 50°C
Injection Rate Fast
Back Pressure 0.500 - 1.50MPa
Screw Speed 50 - 100rpm
Cushion 3.00 - 20.0mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
Note Message
1 .Method B
Resin Grade Manufacturer Category Trademark
TAFMER™ P-0680 Mitsui Chemicals America, Inc. PAO TAFMER™
Ultra Purge HS Moulds Plus International USA, Inc. Proprietary Ultra Purge
4LOY® 10E27200 FR1 4Plas PC+ABS 4LOY®
BCC Resins MB8250 BCC Products Inc. PUR, Unspecified BCC Resins
Baytec® MS-080 (BDO) Covestro - PUR PUR-Ester/MDI Baytec®