PEEK, unreinforced |
General Information | |
---|---|
Resin ID (ISO 1043) |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.30 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.3 | % | |
Flow | 1.0 | % | |
Water Absorption (Saturation, 23°C) | 0.070 | % | Internal Method |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 3100 | MPa | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 11 | kJ/m² | ISO 179/1eA |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 150 | °C | ISO 75-2/A |
Melting Temperature 1 | 343 | °C | ISO 11357-3 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+16 | ohms·cm | IEC 60093 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flammability Classification (0.800 mm) | V-0 | IEC 60695-11-10, -20 |
Note Message | |
---|---|
1 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 4685 | RTP Company | SPS | RTP |
Uniflon GM 800 | UNIFLON | PTFE | Uniflon |
GLS 422-126 | PolyOne Corporation | TPE | GLS |
MAJORIS AFR280 - 8229 | AD majoris | PP Copolymer | MAJORIS |
Delas 170 | Shanghai Lin Gen Rubber Materials Co., Ltd. | PVC+NBR | Delas |