TECHNYL STAR™ SX 216 L2 V60 NATURAL

Category: Nylon 6 , Polyamide 6
Manufacturer: Solvay Engineering Plastics
Trademark: TECHNYL STAR™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: rGqqbD_TECHNYL-STAR-SX-216-L2-V60-NATURAL.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
TECHNYLSTAR polyamide reinforced with 60% of glass fibre, UV stabilized and characterized by a high fluidity of the melt, for injection moulding.
General Information
Filler / Reinforcement
  • Glass Fiber, 60% Filler by Weight
Additive
  • UV Stabilizer
Features
  • Good Moldability
  • Good Surface Finish
  • Good UV Resistance
  • High Flow
  • High Stiffness
Uses
  • Automotive Applications
  • Automotive Interior Parts
Appearance
  • Natural Color
Processing Method
  • Injection Molding
Part Marking Code (ISO 11469)
  • >PA6-GF60<
PhysicalNominal ValueUnitTest Method
Density 1.68g/cm³ISO 1183/A
MechanicalNominal ValueUnitTest Method
Tensile Modulus 18700MPaISO 527-2/1A
Tensile Stress (Break)220MPaISO 527-2/1A
Tensile Strain (Break)2.5%ISO 527-2/1A
ImpactNominal ValueUnitTest Method
Charpy Notched Impact Strength 15kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength 83kJ/m²ISO 179/1eU
Notched Izod Impact Strength 20kJ/m²ISO 180/1A
Unnotched Izod Impact Strength 81kJ/m²ISO 180
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature
    0.45 MPa, Unannealed 220°CISO 75-2/Bf
    1.8 MPa, Unannealed 212°CISO 75-2/Af
Melting Temperature 222°CISO 11357-3
InjectionNominal ValueUnit
Drying Temperature 80.0°C
Suggested Max Moisture 0.15%
Rear Temperature 220 to 225°C
Middle Temperature 235 to 240°C
Front Temperature 240 to 245°C
Mold Temperature 80.0°C
Resin Grade Manufacturer Category Trademark
RTP 2800 B-85A FR A UV RTP Company TPO (POE) RTP
RTV-2 XP-382 Silicones, Inc. Silicone Rubber, RTV-2 RTV-2
SILVER® SA-1350 Guangdong Silver Age Sci & Tech. Co., Ltd SBS SILVER®
CoolPoly® E3603 Celanese Corporation PPA CoolPoly®
LUVOCOM® 20-0916 VP LEHVOSS Group PPA LUVOCOM®