Monprene® IN-22940D (PRELIMINARY DATA)

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Monprene®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: r2qI7S_MonpreneIN22940DPRELIMINARYDATA.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Monprene IN-22940D is a high performance thermoplastic elastomer, available in BLK or NAT, designed for industrial applications. Monprene IN-22940D is a high hardness, low density, UV stabilized grade that is suitable for both injection molding and extrusion.
General Information
Features
  • Low Specific Gravity
  • Without Fillers
  • Low density
  • Light stabilization
  • Good UV resistance
  • Workability, good
  • Good coloring
  • Good adhesion
  • Low liquidity
  • Good chemical resistance
  • Good weather resistance
  • Good toughness
  • High hardness
  • Elastic
Uses
  • Plug
  • Washer
  • Industrial application
  • Rubber substitution
  • Consumer goods application field
  • Profile
  • Knob
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
  • Natural color
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Density 0.900g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)3.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shore D, 1 second, injection molding 42ASTM D2240
    Shore D, 5 seconds, injection molding 40ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress 1ASTM D412
    Transverse flow : 100% strain 7.60MPaASTM D412
    Flow : 100% strain 10.5MPaASTM D412
    Transverse flow : 300% strain 8.21MPaASTM D412
    Flow : 300% strain 11.4MPaASTM D412
Tensile Strength 2ASTM D412
    Transverse flow : Fracture 15.4MPaASTM D412
    Flow : Fracture 316.6MPaASTM D412
    Flow : Fracture 12.5MPaASTM D412
Tensile Elongation 4ASTM D412
    Transverse flow : Fracture 830%ASTM D412
    Flow : Fracture 5690%ASTM D412
    Flow : Fracture 460%ASTM D412
Compression Set 6ASTM D395B
    23°C, 22 hr 53%ASTM D395B
    70°C, 22 hr 89%ASTM D395B
Fill AnalysisNominal ValueUnitTest Method
Apparent Viscosity (200°C, 206 sec^-1)360Pa·sASTM D3835
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Rear Temperature 216 - 238°C
Middle Temperature 216 - 238°C
Front Temperature 216 - 238°C
Nozzle Temperature 216 - 238°C
Processing (Melt) Temp 216 - 238°C
Mold Temperature 16 - 32°C
Injection Pressure 1.38 - 6.89MPa
Injection Rate Moderate-Fast
Back Pressure 0.172 - 0.345MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 204 - 227°C
Cylinder Zone 2 Temp. 204 - 227°C
Cylinder Zone 3 Temp. 204 - 227°C
Cylinder Zone 4 Temp. 204 - 227°C
Cylinder Zone 5 Temp. 204 - 227°C
Die Temperature 204 - 227°C
Extrusion instructions
螺杆转速30 - 100 rpm
Note Message
1 .C mold, 510mm/min
2 .C mold, 510mm/min
3 .Extruded tape
4 .C mold, 510mm/min
5 .Extruded tape
6 .Type 1
Resin Grade Manufacturer Category Trademark
RONFALIN® CP55 A. Schulman Europe ABS RONFALIN®
NILAMID® A3 GF50 Nilit Plastics Nylon 66 NILAMID®
Boda BDF-KR2752 Chenguang Fluoro & Silicone Elastomers Co., Ltd. Fluorelastomer Boda
Exac FEP Saint Gobain - Norton FEP Exac
Hypro® PPC-CC30 NATURAL Entec Polymers PP Copolymer Hypro®