Monprene®OM-10275 is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Monprene®The main characteristics of the OM-10275 are: resistance to sunlight.

Typical application areas include:
  • Handle
  • engineering/industrial accessories
  • Electrical/electronic applications
  • electrical appliances
  • Tools
General Information
Features
  • Sunlight Resistant
  • Without Fillers
  • smoothness
  • Light stabilization
  • Medium liquidity
  • Lubrication
  • Medium density
  • Medium hardness
  • UV absorption
Uses
  • Handle
  • overmolding
  • Electrical appliances
  • Power/other tools
  • Soft handle
  • Mobile phone
  • Sporting goods
  • Stationery
  • Knob
  • Dental application field
  • Toothbrush handle
  • Bonding
Appearance
  • Opacity
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.998g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)7.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shore A, 1 second, injection molding 65ASTM D2240
    Shore A, 1 second, injection molding 178ASTM D2240
    Shore A, 5 seconds, injection molding 275ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    Transverse flow : 100% strain 33.12MPaASTM D412
    Flow : 100% strain 44.78MPaASTM D412
    Transverse flow : 300% strain 55.05MPaASTM D412
    Flow : 300% strain 66.47MPaASTM D412
Tensile Strength 7ASTM D412
    Transverse flow : Fracture 8.20MPaASTM D412
    Flow : Fracture 9.88MPaASTM D412
Tensile Elongation 8ASTM D412
    Transverse flow : Fracture 580%ASTM D412
    Flow : Fracture 660%ASTM D412
Tear Strength 9ASTM D624
    Transverse flow 45.9kN/mASTM D624
    Flow 53.1kN/mASTM D624
Compression Set 10ASTM D395B
    23°C, 22 hr 47%ASTM D395B
    70°C, 22 hr 90%ASTM D395B
Additional InformationNominal Value
Adhesion to ABS
Adhesion to PC
Adhesion to PC/ABS
InjectionNominal ValueUnit
Drying Temperature 60.0°C
Drying Time 2.0 - 4.0hr
Rear Temperature 138 - 160°C
Middle Temperature 182 - 199°C
Front Temperature 182 - 199°C
Nozzle Temperature 193 - 210°C
Processing (Melt) Temp 177 - 199°C
Mold Temperature 4.44 - 48.9°C
Injection Pressure 1.38 - 5.52MPa
Back Pressure 0.172 - 0.862MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
潮湿会使材料降解。建议进行干燥处理。可以把材料放入除湿干燥机,在140°F的温度下干燥2-4小时。
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 138 - 149°C
Cylinder Zone 2 Temp. 149 - 160°C
Cylinder Zone 3 Temp. 160 - 182°C
Cylinder Zone 5 Temp. 171 - 193°C
Die Temperature 182 - 204°C
Note Message
1 .Aging 48 hr
2 .Aging 48 hr
3 .Mouth die C, 510mm/min
4 .Mouth die C, 510mm/min
5 .C mold, 510mm/min
6 .C mold, 510mm/min
7 .C mold, 510mm/min
8 .Mouth die C, 510mm/min
9 .C mold, 510mm/min
10 .Type 1
Resin Grade Manufacturer Category Trademark
Mecoline I RDX 1223 F Melos GmbH TP, Unspecified Mecoline
Colorite 12 Series 9512 Colorite Polymers PVC, Unspecified Colorite 12 Series
Etinox® EI-6530 Ercros, S.A. PVC, Flexible Etinox®
Kepital® GD-52 Korea Engineering Plastics Co., Ltd Acetal (POM) Copolymer Kepital®
LUVOCOM® 1-0889-5/RD Lehmann & Voss & Co. Nylon 66 LUVOCOM®