Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Teknor Apex Company (Chem Polymer) |
Trademark: | Chemlon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | qx3ptS_Chemlon-225-15-MG.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Chemlon® 225-15 MG is a Polyamide 6 (Nylon 6) material filled with 15% glass fiber and 25% mineral. It is available in Asia Pacific, Europe, or North America for injection molding. Primary attribute of Chemlon® 225-15 MG: Flame Rated. Typical application of Chemlon® 225-15 MG: Automotive |
General Information | |
---|---|
Filler / Reinforcement |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.52 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 0.15 to 0.40 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 128 | MPa | ASTM D638 |
Tensile Elongation | ASTM D638 | ||
Yield | 2.5 | % | |
Break | 2.5 | % | |
Flexural Modulus | 7580 | MPa | ASTM D790 |
Flexural Strength | 190 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 85 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 205 | °C | ASTM D648 |
Melting Temperature | 216 | °C | DSC |
CLTE - Flow | 5.5E-5 | cm/cm/°C | ASTM D696 |
RTI Elec | UL 746 | ||
0.810 mm | 65.0 | °C | |
1.50 mm | 65.0 | °C | |
3.00 mm | 65.0 | °C | |
RTI Imp | UL 746 | ||
0.810 mm | 65.0 | °C | |
1.50 mm | 65.0 | °C | |
3.00 mm | 65.0 | °C | |
RTI Str | UL 746 | ||
0.810 mm | 65.0 | °C | |
1.50 mm | 65.0 | °C | |
3.00 mm | 65.0 | °C |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+14 | ohms·cm | ASTM D257 |
Dielectric Strength (3.00 mm) | 12 | kV/mm | ASTM D149 |
Comparative Tracking Index (CTI) | 500 | V | UL 746 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (0.810 mm) | HB | UL 94 | |
Oxygen Index | 24 | % | ASTM D2863 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Suggested Max Moisture | 0.20 | % | |
Suggested Max Regrind | 25 | % | |
Rear Temperature | 218 to 235 | °C | |
Middle Temperature | 246 to 257 | °C | |
Front Temperature | 246 to 268 | °C | |
Nozzle Temperature | 246 to 268 | °C | |
Processing (Melt) Temp | 249 to 266 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Prixene® EB070E17 | POLYMAT | LDPE | Prixene® |
Axiall PVC 10756 | Axiall Corporation | PVC, Flexible | Axiall PVC |
Fainplast PVC FK 90 | Fainplast Compounds S.r.l | PVC, Unspecified | Fainplast PVC |
EpoxAcoat® Red | Smooth-On, Inc | Epoxy | EpoxAcoat® |
Hylon® N1020HLUV2 | Ravago Manufacturing Americas, LLC | Nylon 66 | Hylon® |