Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | PENTAC Polymer GmbH |
Trademark: | PENTAMID A |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | qbTtzV_PENTAMIDAGV35HYD2RCblack.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Normal viscosity, hydrolysis stabilised polyamide 66, 35% glass fiber reinforced, ReCompound |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Recycled Content |
|
Features |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.41 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Transverse flow | 0.70 | -- | % | ISO 294-4 |
Flow | 0.45 | -- | % | ISO 294-4 |
Water Absorption | ISO 62 | |||
Saturated, 23°C | 4.9 | -- | % | ISO 62 |
Equilibrium, 23°C, 50% RH | 1.3 | -- | % | ISO 62 |
Viscosity Number | 130 | -- | cm³/g | ISO 307 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 10500 | 8400 | MPa | ISO 527-2/1 |
Tensile Stress (Break) | 175 | 135 | MPa | ISO 527-2/5 |
Tensile Strain (Break) | 3.5 | 5.0 | % | ISO 527-2/5 |
Flexural Modulus | 9300 | -- | MPa | ISO 178 |
Flexural Stress | 240 | -- | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 11 | 16 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 75 | 85 | kJ/m² | ISO 179/1eU |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, not annealed | 255 | -- | °C | ISO 75-2/B |
1.8 MPa, not annealed | 240 | -- | °C | ISO 75-2/A |
Melting Temperature | 260 | -- | °C | ISO 11357-3 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Dielectric Strength | 30 | -- | kV/mm | IEC 60243-1 |
Dielectric Constant (1 MHz) | 3.50 | -- | IEC 60250 | |
Comparative Tracking Index | 425 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (3.2 mm) | HB | -- | UL 94 |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Shortname | PA66, MHWRC, 14-100, GF35 | -- | ISO 1874 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Drying Time | 3.0 | hr | |
Suggested Max Moisture | 0.050 - 0.13 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 275 - 295 | °C | |
Middle Temperature | 280 - 305 | °C | |
Front Temperature | 285 - 295 | °C | |
Processing (Melt) Temp | 270 - 310 | °C | |
Mold Temperature | 60 - 100 | °C | |
Injection Pressure | 76.0 | MPa | |
Screw L/D Ratio | 18.0:1.0 to 22.0:1.0 | ||
Screw Compression Ratio | 2.2:1.0 to 2.8:1.0 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Telcar® TL-8431 | Teknor Apex Company | TPE | Telcar® |
NEFTEKHIM PP 1520H (S38F) | Nizhnekamskneftekhim Inc. | PP Homopolymer | NEFTEKHIM PP |
DENITER C 3010 | Vamp Tech | PC+PBT | DENITER |
Fainplast PVC RK 218 | Fainplast Compounds S.r.l | PVC, Rigid | Fainplast PVC |
OnForce™ LFT SF-40LCF/000 Black | PolyOne Corporation | PPS | OnForce™ LFT |