Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | PENTAC Polymer GmbH |
Trademark: | PENTAMID A |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | qIMgOs_PENTAMIDAGV25Hblue50101.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Normal viscosity, heat stabilised polyamide 66, 25% glass fiber reinforced, Special Pigmentation |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.32 | -- | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Transverse flow | 0.90 | -- | % | ISO 294-4 |
Flow | 0.60 | -- | % | ISO 294-4 |
Water Absorption | ISO 62 | |||
Saturated, 23°C | 6.2 | -- | % | ISO 62 |
Equilibrium, 23°C, 50% RH | 2.1 | -- | % | ISO 62 |
Viscosity Number | 140 | -- | cm³/g | ISO 307 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 8200 | 5600 | MPa | ISO 527-2/1 |
Tensile Stress (Break) | 150 | 105 | MPa | ISO 527-2/5 |
Tensile Strain (Break) | 3.3 | 6.0 | % | ISO 527-2/5 |
Flexural Modulus | 7100 | -- | MPa | ISO 178 |
Flexural Stress | 190 | -- | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 8.0 | 10 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 50 | 70 | kJ/m² | ISO 179/1eU |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
0.45 MPa, not annealed | 245 | -- | °C | ISO 75-2/B |
1.8 MPa, not annealed | 220 | -- | °C | ISO 75-2/A |
Melting Temperature | 260 | -- | °C | ISO 11357-3 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Dielectric Strength | 32 | -- | kV/mm | IEC 60243-1 |
Dielectric Constant (1 MHz) | 3.50 | -- | IEC 60250 | |
Comparative Tracking Index | 450 | -- | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (3.2 mm) | HB | -- | UL 94 |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Shortname | PA66, MHRC, 14-080 N, GF25 | -- | ISO 1874 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Drying Time | 3.0 | hr | |
Suggested Max Moisture | 0.060 - 0.14 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 265 - 285 | °C | |
Middle Temperature | 270 - 290 | °C | |
Front Temperature | 275 - 285 | °C | |
Processing (Melt) Temp | 265 - 295 | °C | |
Mold Temperature | 60 - 100 | °C | |
Injection Pressure | 70.0 | MPa | |
Screw L/D Ratio | 18.0:1.0 to 22.0:1.0 | ||
Screw Compression Ratio | 2.2:1.0 to 2.8:1.0 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
ASTALON™ K2000UR | Marplex Australia Pty. Ltd. | PC | ASTALON™ |
Cevian® AF800 | Daicel Polymer Ltd. | ABS | Cevian® |
Hypro® PPC-GF10 NATURAL | Entec Polymers | PP Impact Copolymer | Hypro® |
Kepital® TE-23S | KEP Americas | Acetal (POM) Copolymer | Kepital® |
APEX® S-96-A0914N-90 | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | APEX® |