Category: | PPA , Polyphthalamide |
Manufacturer: | RTP Company |
Trademark: | RTP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | ppt0U4_RTP-4099-X-94115.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Impact Modified - Glass Fiber - Heat Stabilized |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
RoHS Compliance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.20 mm) | 0.40 - 0.70 | % | ASTM D955 |
Moisture Content | 0.050 | % |
Additional Information | Nominal Value | Unit | |
---|---|---|---|
Primary Additive | 15 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 4140 | MPa | ASTM D638 |
Tensile Strength | 75.8 | MPa | ASTM D638 |
Tensile Elongation (Yield) | 4.0 - 6.0 | % | ASTM D638 |
Flexural Modulus | 4140 | MPa | ASTM D790 |
Flexural Strength | 117 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.20 mm) | 210 | J/m | ASTM D256 |
Unnotched Izod Impact (3.20 mm) | 850 | J/m | ASTM D4812 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 107 | °C | |
Drying Time | 4.0 - 6.0 | hr | |
Dew Point | -31.7 | °C | |
Processing (Melt) Temp | 288 - 302 | °C | |
Mold Temperature | 121 - 149 | °C | |
Injection Pressure | 68.9 - 124 | MPa |
Injection instructions |
---|
Desiccant Type Dryer Required. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Moplen HP401R | LyondellBasell Industries | PP Homopolymer | Moplen |
Bergamid™ B70 G30 GR177 | PolyOne Corporation | Nylon 6 | Bergamid™ |
GAPEX® RPP30DA13NA | Ferro Corporation | PP Homopolymer | GAPEX® |
LUVOCOM® 1105-9012/T | Lehmann & Voss & Co. | PEEK | LUVOCOM® |
ESTOPLAST EP 4020WW26 | Ester Industries Ltd. | PBT | ESTOPLAST EP |