General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.43 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.18 mm) | 0.12 | % | ASTM D955 |
Water Absorption (23°C, 24 hr) | 0.14 | % | ASTM D570 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 119 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 9650 | MPa | ASTM D638 |
Tensile Strength | 141 | MPa | ASTM D638 |
Tensile Elongation (Break) | 4.7 | % | ASTM D638 |
Flexural Modulus | 6890 | MPa | ASTM D790 |
Flexural Strength | 207 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 210 | J/m | ASTM D256 |
Unnotched Izod Impact (3.18 mm) | 1200 | J/m | ASTM D4812 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 82.2 | °C | ASTM D648 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Dielectric Strength | 20 | kV/mm | ASTM D149 |
Dielectric Constant (1 MHz) | 3.70 | ASTM D150 | |
Dissipation Factor (1 MHz) | 0.012 | ASTM D150 |
Additional Information |
---|
Mold Shrinkage, Linear-Flow, ASTM D955, 0.25in.: 2.4mil/in. |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 107 | °C | |
Drying Time | 6.0 | hr | |
Suggested Max Moisture | 0.010 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 218 - 274 | °C | |
Middle Temperature | 218 - 274 | °C | |
Front Temperature | 218 - 274 | °C | |
Nozzle Temperature | 229 - 274 | °C | |
Mold Temperature | 23.9 - 121 | °C | |
Injection Pressure | 68.9 - 103 | MPa | |
Clamp Tonnage | 5.5 - 11 | kN/cm² |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
S&E PVC GPT 150 | S&E Specialty Polymers, LLC | PVC, Unspecified | S&E PVC |
Tecomid® NB40 MR25 NL IL | Eurotec Engineering Plastics | Nylon 6 | Tecomid® |
XYRON™ X551V | Asahi Kasei Chemicals Corporation | PPE+PS | XYRON™ |
Axpoly® r-PP51 1079 | Axion Polymers | PP Copolymer | Axpoly® |
EMERGE™ PC 8210-31 | Trinseo | PC | EMERGE™ |