IROGRAN® A 92 E 4738

Category: TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester)
Manufacturer: Huntsman Corporation
Trademark: IROGRAN®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: pR6GIq_IROGRAN-A-92-E-4738.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection moulding applications.

Additional characteristics of the product are flexibility and high mechanical resistance.

PERFORMANCE FEATURES
  • High oil resistance
  • Good melt flow
  • High wear resistance
  • Dynamically highly loadable
  • Low-temperature flexibility

APPLICATIONS
For the production of tooth belts, round cordsprofiles, high pressure hoses.
General Information
Features
  • Flexibility at low temperatures
  • Good liquidity
  • Good flexibility
  • Good wear resistance
  • Oil resistance
Uses
  • Conveyor belt repair
  • Pipe
RoHS Compliance
  • Contact manufacturer
Appearance
  • White
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.20g/cm³
Melt Volume-Flow Rate (MVR) (220°C/10.0 kg)40.0cm³/10minInternal method
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240, ISO 868
    Shore A, Injection Molding 92ASTM D2240, ISO 868
    Shore D, Injection Molding 41ASTM D2240, ISO 868
MechanicalNominal ValueUnitTest Method
Abrasion 25mm³ISO 4649
ElastomersNominal ValueUnitTest Method
Tensile Stress 1DIN 53504
    100% strain 8.00MPaDIN 53504
    300% strain 24.0MPaDIN 53504
Tensile Stress 2(Break)55.0MPaDIN 53504
Tensile Elongation 3(Break)450%DIN 53504
Tear Strength 4110kN/mISO 34-1
Compression Set 5ASTM D395, ISO 815
    23°C, 24 hr 25%ASTM D395, ISO 815
    70°C, 24 hr 40%ASTM D395, ISO 815
InjectionNominal ValueUnit
Drying Temperature
    -- 100 - 110°C
    Vacuum dryer 80.0 - 90.0°C
Drying Time
    -- 3.0hr
    Vacuum dryer 3.0hr
Dew Point -30.0°C
Rear Temperature 175 - 195°C
Middle Temperature 175 - 195°C
Front Temperature 175 - 195°C
Nozzle Temperature 180 - 200°C
Mold Temperature 20.0 - 70.0°C
ExtrusionNominal ValueUnit
Drying Temperature 100 - 110°C
Drying Time 3.0hr
Hopper Temperature 25.0 - 40.0°C
Cylinder Zone 1 Temp. 165 - 190°C
Cylinder Zone 2 Temp. 165 - 190°C
Cylinder Zone 3 Temp. 165 - 190°C
Cylinder Zone 4 Temp. 165 - 190°C
Cylinder Zone 5 Temp. 165 - 190°C
Adapter Temperature 175 - 195°C
Die Temperature 175 - 200°C
Extrusion instructions
Nozzle: 170 to 200°C
Note Message
1 .Injection Molded
2 .Injection Molded
3 .Injection Molded
4 .Injection Molded
5 .Injection Molded
Resin Grade Manufacturer Category Trademark
MarFlex® 9659 Chevron Phillips Chemical Company LLC HDPE MarFlex®
RTP ESD 683 RTP Company ABS RTP
T-Blend® 6594B-G80E-A TSRC Corporation SEBS T-Blend®
4LOY® 10E17400 I 4Plas PC+ABS 4LOY®
Glastic® SG-200 Glastic Corporation Polyester, TS Glastic®