Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Teknor Apex Company |
Trademark: | Sarlink® TPV |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | on5fKT_Sarlink-TPV-2555.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Sarlink®TPV 2555 is a thermoplastic vulcanized rubber (TPV) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Sarlink®The main characteristics of TPV 2555 are: flame retardant/rated flame. Typical application areas include:
|
General Information | |
---|---|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.948 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 0.60 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A | 60 | ASTM D2240 | |
Shaw A, 5 seconds | 55 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | ASTM D412 | ||
Transverse flow : Fracture | 4.62 | MPa | ASTM D412 |
Flow : Fracture | 4.34 | MPa | ASTM D412 |
Tensile Elongation | ASTM D412 | ||
Transverse flow : Fracture | 320 | % | ASTM D412 |
Flow : Fracture | 270 | % | ASTM D412 |
Tear Strength | 15.8 | kN/m | ASTM D624 |
Compression Set (100°C, 22 hr) | 29 | % | ASTM D395 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air - Across Flow (135°C, 24 hr) | 3.0 | % | ASTM D573 |
Change in Ultimate Elongation in Air (135°C, 24 hr) | 7.0 | % | ASTM D573 |
Change in Durometer Hardness in Air (support a, 135°C, 24 hr) | 60 | ASTM D573 | |
rate of change in tensile strength- Transverse flow (23°C, 70 hr, in IRM 903 oil) | 22 | % | ASTM D471 |
rate of change of ultimate elongation- Transverse flow (23°C, 70 hr, in IRM 903 oil) | 32 | % | ASTM D471 |
Change in Volume (25°C, 70 hr, in IRM 903 oil) | 23 | % | ASTM D471 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -60.0 | °C | ASTM D746 |
RTI Elec | 50.0 | °C | UL 746 |
RTI Imp | 50.0 | °C | UL 746 |
RTI | 50.0 | °C | UL 746 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (1.50 mm, Natural and Black Colors) | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 173 - 213 | °C | |
Middle Temperature | 179 - 219 | °C | |
Front Temperature | 184 - 224 | °C | |
Nozzle Temperature | 190 - 230 | °C | |
Processing (Melt) Temp | 190 - 230 | °C | |
Mold Temperature | 35.0 - 60.0 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Fast | ||
Back Pressure | 0.172 - 0.862 | MPa | |
Screw Speed | 50 - 120 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 166 - 204 | °C | |
Cylinder Zone 2 Temp. | 171 - 210 | °C | |
Cylinder Zone 3 Temp. | 177 - 216 | °C | |
Cylinder Zone 5 Temp. | 182 - 221 | °C | |
Die Temperature | 190 - 227 | °C |
Extrusion instructions |
---|
螺杆转速30 - 100 rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 600 FR AB | RTP Company | ABS | RTP |
VENYL UFRHGR208R - 8229 | AD majoris | Nylon 66 | VENYL |
Zythane® 6075D | Alliance Polymers & Services | TPU-Polyether | Zythane® |
Electrafil® PP-61/EC | Techmer Engineered Solutions | PP Copolymer | Electrafil® |
Grilamid® LBV-65H FWA black 9225 | EMS-GRIVORY | Nylon 12 | Grilamid® |