Leona™ 9400S is a Polyamide 66 (Nylon 66) product. It is available in Africa & Middle East, Asia Pacific, Europe, or North America. Applications of Leona™ 9400S include engineering/industrial parts, film, housings and industrial applications. Characteristics include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Specific Gravity | 1.14 | -- | g/cm³ | ASTM D792, ISO 1183 |
Water Absorption | ||||
Saturation, 23°C | -- | 2.8 | % | |
Equilibrium, 23°C, 50% RH | -- | 2.8 | % | ISO 62 |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Rockwell Hardness | ||||
M-Scale | 75 | -- | ASTM D785 | |
M-Scale | 80 | -- | ISO 2039-2 | |
R-Scale | 120 | -- | ISO 2039-2 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 2700 | 700 | MPa | ISO 527-2 |
Tensile Stress | ||||
Yield, 23°C | 80.0 | 40.0 | MPa | ISO 527-2 |
-- | 79.0 | 44.0 | MPa | ASTM D638 |
Tensile Strain | ||||
Yield, 23°C | 4.0 | 22 | % | ISO 527-2 |
Break | 60 | 260 | % | ASTM D638 |
Break, 23°C | -- | > 100 | % | ISO 527-2 |
Flexural Modulus | ||||
-- | 2600 | 800 | MPa | ASTM D790 |
23°C | 2300 | 700 | MPa | ISO 178 |
Flexural Strength | ||||
-- | 108 | 44.0 | MPa | ASTM D790 |
23°C | 97.0 | 30.0 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | 7.0 | 41 | kJ/m² | ISO 179 |
Charpy Unnotched Impact Strength | No Break | No Break | ISO 179 | |
Notched Izod Impact | 54 | 270 | J/m | ASTM D256 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Deflection Temperature Under Load | ||||
0.45 MPa, Unannealed | 190 | -- | °C | ASTM D648 |
0.45 MPa, Unannealed | 165 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 60.0 | -- | °C | ISO 75-2/A |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 1.0E+14 | -- | ohms | ASTM D257, IEC 60093 |
Volume Resistivity | ||||
-- | 1.0E+15 | -- | ohms·cm | ASTM D257 |
23°C | 1.0E+15 | -- | ohms·cm | IEC 60093 |
Dielectric Strength | 20 | -- | kV/mm | ASTM D149, IEC 60243-1 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 2281 LF TFE 10 | RTP Company | PEEK | RTP |
SCHULAMID® 612 FS 5003 MC | A. Schulman Europe | Nylon 612 | SCHULAMID® |
SCANAMID 6 B12^ F45 | Polykemi AB | Nylon 6 | SCANAMID 6 |
Synthos EPS® 0513S/CZ | Synthos S.A. | PS (EPS) | Synthos EPS® |
MAJORIS CW214 | AD majoris | PP, Unspecified | MAJORIS |