Fluoroelastomer Rubber, 76-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK810, A1-10, B37, B38, EF31, EO78, F15, Z1. Where Z1 = compression set 30% max. ASTM designation = FKM. ISO designation = FPM. Excellent resistance to oils, fuels and hydraulic fluids at high temperature. |
General Information | |
---|---|
Features |
|
Agency Ratings |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
IRHD Hardness | 80 | ASTM D1415, ISO 48 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield) | 11.0 | MPa | ASTM D412, ISO 37 |
Tensile Elongation (Break) | 150 | % | ASTM D412, ISO 37 |
Compression Set (200°C, 24 hr) | 14 | % | ASTM D395B, ISO 815 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (250°C, 72 hr) | -25 | % | ASTM D412, ISO 37 |
Change in Ultimate Elongation in Air (250°C, 72 hr) | -25 | % | ASTM D412, ISO 37 |
Change in IRHD Hardness in Air (250°C, 72 hr) | 10 | ASTM D573, ISO 188 |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Maximum Operating Temperature | 200 | °C |
Additional Information |
---|
Minimum Operating Temperature: -20°C (-4°F) |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Santoprene™ 121-58W175 | ExxonMobil Chemical | TPV | Santoprene™ |
ADPOLY BP-402 | Lotte Chemical Corporation | PP, Unspecified | ADPOLY |
Dynaprene® VE0064A | Nantex Industry Co., Ltd. | TPE | Dynaprene® |
Hipolyene 8021 T | Zylog Plastalloys | TPO (POE) | Hipolyene |
Infino EN-1052 | SAMSUNG SDI CO., LTD. | PC | Infino |